Ebonite (Hard Rubber)

Vulcanised rubber is rubber with a few sulphur bridges between its chains. Keep adding sulphur and the bridges multiply until the chains cannot move at all: the soft, stretchy material turns into a hard black solid you can turn on a lathe, polish like ebony and use as an electrical insulator. **US 8,075**, "Improvement in the Manufacture of India Rubber", Nelson Goodyear (brother of Charles), granted 6. May 1851, claims "the combining of india-rubber and sulphur… for making a hard and inflexible substance hitherto unknown": about equal parts by weight, heated to 260–275 °F for three to six hours. It was one of the first rigid materials made by chemically changing a natural polymer, over half a century before Bakelite. **You turn a part from commercial ebonite rod and measure what the sulphur did** — its density, and its charge when rubbed. Curing ebonite needs a heated press and releases hydrogen sulphide, so the blueprint starts from finished rod; the notebook does the chemistry.
Intermedio
3 hours

Instrucciones

1

Cut the blank

Clamp 20 mm ebonite rod in the vise between soft jaws. Saw off 60 mm. Ebonite chips like hard wood; saw slowly to avoid cracking the end.

Materiales para este paso:

Varilla de ebonitaVarilla de ebonita1 pieza

Herramientas necesarias:

Sierra para metalesSierra para metales
Tornillo de bancoTornillo de banco
Regla de aceroRegla de acero
Gafas de seguridad transparentesGafas de seguridad transparentes
2

Chuck and face

Grip 20 mm of the blank in the lathe's 3-jaw chuck. Face the end square with a sharp HSS tool at about 800 rpm, light cuts.

Herramientas necesarias:

Torno de metalTorno de metal
Juego de herramientas de torno (HSS)Juego de herramientas de torno (HSS)
Gafas de seguridad transparentesGafas de seguridad transparentes
Mascarilla antipolvoMascarilla antipolvo
3

Turn to 16 mm

Turn 40 mm of length down to 16.0 mm. Check with the caliper every pass. The chips smell of sulphur - that is the bonded sulphur you measure later.

Herramientas necesarias:

Torno de metalTorno de metal
Juego de herramientas de torno (HSS)Juego de herramientas de torno (HSS)
Calibre digital de 6 pulgadasCalibre digital de 6 pulgadas
4

Drill the bore

Spot the centre with a centre drill, then drill 3 mm through 35 mm from the tailstock. Clear chips every 5 mm - ebonite heats and gums if packed.

Herramientas necesarias:

Juego de brocas de centrarJuego de brocas de centrar
Juego de brocas en estuche índiceJuego de brocas en estuche índice
Torno de metalTorno de metal
5

Taper the grip

Set the compound to a shallow angle and taper 25 mm from 16 mm down to 10 mm. This is a fountain-pen grip section, the job ebonite still does today.

Herramientas necesarias:

Torno de metalTorno de metal
Juego de herramientas de torno (HSS)Juego de herramientas de torno (HSS)
Calibre digital de 6 pulgadasCalibre digital de 6 pulgadas
6

Sand and polish

At low speed, sand 400 then 800 grit, then run the Micro-Mesh grits in order. Finish with polishing compound on a cloth. Ebonite takes a deep gloss without lacquer.

Materiales para este paso:

Papel de lijaPapel de lija2 hojas
Pasta de pulirPasta de pulir5 g

Herramientas necesarias:

Kit de lijado de micromalla (9 granos)Kit de lijado de micromalla (9 granos)
Torno de metalTorno de metal
Mascarilla antipolvoMascarilla antipolvo
7

Part off

Part off at 45 mm with the parting tool. Chamfer the cut end by hand with 800 grit.

Herramientas necesarias:

Juego de herramientas de torno (HSS)Juego de herramientas de torno (HSS)
Torno de metalTorno de metal
8

Measure the density

Weigh the part. Drop it into 50 ml of water in the graduated cylinder and read the rise. Do the same with a bundle of rubber bands. Enter both in the notebook.

Materiales para este paso:

Gomas elásticasGomas elásticas1 paquete

Herramientas necesarias:

Báscula digital de precisiónBáscula digital de precisión
Probeta graduadaProbeta graduada
9

Rub it and pick up paper

Tear tissue into 5 mm scraps. Rub the ebonite 10 strokes on wool felt and hold it 2 cm above the scraps. Repeat with an acrylic offcut. Count scraps lifted by each.

Materiales para este paso:

Papel de seda sin ácidoPapel de seda sin ácido1 hoja
Lámina de acrílicoLámina de acrílico1 pieza

Herramientas necesarias:

Fieltro de lanaFieltro de lana
10

The sulphur arithmetic

Cargando el cuaderno de Jupyter…
11

History & Context

**What the patent specifies:** rubber and sulphur in about equal parts (or 2 : 1 with magnesia or lime), 260–275 °F, three to six hours. **Modern build (derived):** commercial ebonite rod, typically 25–32 % sulphur - the notebook shows why more than about 32 % cannot bond. Ebonite was named for ebony, which it replaced in combs, pipe stems and instrument parts. It became a standard insulator of the electrical age and is still preferred for fountain-pen feeds because ink wets it. Its limits: it softens with heat, fades to brown and smells of sulphur in sunlight as the surface oxidises, and is brittle under impact.

Materiales

6

Herramientas requeridas

14

Blueprints relacionados

Estos blueprints comparten conocimiento — técnicas, materiales o principios

CC0 Dominio público

Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.

Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.

Discusión

(0)

Iniciar sesión para unirte a la discusión

Cargando comentarios...