SENI
KECANTIKAN & KESEJAHTERAAN
KRAFTANGAN
BUDAYA & SEJARAH
HIBURAN
ALAM SEKITAR
MAKANAN & MINUMAN
KEJURUTERAAN TERBALIK
SAINS
SUKAN
TEKNOLOGI
BOLEH PAKAI
Hex Key Set: Hexagonal Steel Drawn, Bent and Hardened
Forge

Dicipta oleh

Forge

14. Oktober 2026NO
22
0
0
0
0

Hex Key Set: Hexagonal Steel Drawn, Bent and Hardened

A hex key is a single rod of hard hexagonal steel bent into an L with one long and one short arm; its blunt ends fit a hexagonal screw socket. The hexagonal rod is made by drawing steel through a hexagonal die, then bent and cut to length. Forge and draw tool steel to a set of sizes, bend, cut, harden and temper. The picture: a set of six L-shaped hex keys.
Lanjutan
Two days

Arahan

1

Forge to hex

Draw tool steel down and forge the larger sizes hexagonal in the swage block with the top swage, as for hex bar.

Bahan untuk langkah ini:

Bar keluli alat segi lapanBar keluli alat segi lapan0.3 kg
ArangArang3 as required

Alatan diperlukan:

Relau tukang besiRelau tukang besi
AndasAndas
Tukul kepala baji lintangTukul kepala baji lintang
Blok acuan berlubangBlok acuan berlubang
Swage atasSwage atas
Penyepit tukang besiPenyepit tukang besi
Sarung tangan kimpalanSarung tangan kimpalan
Cermin mata keselamatanCermin mata keselamatan
2

Draw the small sizes

For the small sizes, point the rod and pull it cold through hexagonal holes in the drawplate, one size smaller each time, with lubricant. Anneal it whenever it gets stiff.

Alatan diperlukan:

Plat tarik keluliPlat tarik keluli
Ragum bangku beratRagum bangku berat
Penyepit tukang besiPenyepit tukang besi
Relau tukang besiRelau tukang besi
Pelincir tarik dawaiPelincir tarik dawai
3

Bend and cut

Bend each rod to 90°, short arm about a third of the long one (our proportion), and saw it to length.

Alatan diperlukan:

Ragum bangku beratRagum bangku berat
Tukul kepala baji lintangTukul kepala baji lintang
Gergaji BesiGergaji Besi
4

Harden and temper

Heat each key to cherry red and quench in water, polish, then temper to blue so it is hard but springy (our temper).

Bahan untuk langkah ini:

AirAir10 liter

Alatan diperlukan:

Relau tukang besiRelau tukang besi
Baldi pelindapkejutanBaldi pelindapkejutan
Penyepit tukang besiPenyepit tukang besi
Sarung tangan kimpalanSarung tangan kimpalan
Cermin mata keselamatanCermin mata keselamatan
5

Square the ends

Grind both ends square and flat, so they sit snugly in the socket. Check each key in a matching socket.

Alatan diperlukan:

Batu canai rodaBatu canai roda
6

Steel for a set

Memuatkan buku nota Jupyter…

Bahan

3
  • Pemegang Tempat
  • 3 as required
    Pemegang Tempat
  • 10 liter
    Pemegang Tempat

Alatan Diperlukan

14

Blueprint berkaitan

Blueprint ini berkongsi pengetahuan — teknik, bahan atau prinsip

CC0 Domain Awam

Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.

Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.

Perbincangan

(0)

Log masuk untuk menyertai perbincangan

Memuatkan komen...