Lightfastness: Which Colours Are Still There in Fifty Years
Some pigments are effectively permanent and some fade visibly within a decade of ordinary daylight. The difference is chemistry, it is known, and it is printed on the tube — and it is the thing beginners ignore most consistently.
The failures are not subtle. A painting whose reds were made with a fugitive lake loses them entirely, leaving the blues and earths behind — which is why so many old paintings look colder than they were painted.
It is also entirely avoidable. Choosing lightfast pigments costs nothing extra at the moment of choosing, and it is the single decision that most determines whether work outlives the person who made it.
Pertengahan
3 hours
Arahan
1
1
Read the tube: pigment index, not colour name
Read the tube: pigment index, not colour name
The colour NAME on a tube means nothing — 'permanent rose' and 'crimson' are marketing, and two makers use them for different chemicals. The COLOUR INDEX number does mean something: PB29 is ultramarine, PR108 is cadmium red, PY35 is cadmium yellow, wherever you buy it.
The lightfastness rating is usually ASTM I to V, or a star system. ASTM I is excellent, II is very good, and III and below should not be used for anything meant to last.
A tube with no pigment index and no lightfastness rating is telling you something. Student ranges frequently substitute cheap fugitive pigments under traditional names, which is legitimate for practice work and not for anything you will still want in twenty years.
Bahan untuk langkah ini:
Set Serbuk Pigmen Tanah1 kepingAlatan diperlukan:
Kanta Pembesar Tukang Emas2
2
What fades, and why
What fades, and why
ORGANIC LAKE pigments — dyes precipitated onto a transparent substrate — are the classic fugitives. Madder lake, carmine from cochineal, and many bright modern pinks and violets fade because the dye molecule itself is broken apart by ultraviolet light.
MINERAL pigments are generally far more stable, because there is nothing to break apart: an iron oxide is already the stable oxidised form. That is why earths, ochres, and the cadmiums and cobalts endure.
There are specific exceptions worth knowing. Vermilion blackens. Lead white darkens in sulphurous air. Prussian blue fades in light and partly recovers in the dark, which is genuinely strange and well documented. Chrome yellow darkens, which is what happened to some of Van Gogh's sunflowers.
Bahan untuk langkah ini:
Set Serbuk Pigmen Tanah1 kepingAlatan diperlukan:
Kanta Pembesar Tukang Emas3
3
Test it yourself: half in the light, half in the dark
Test it yourself: half in the light, half in the dark
Paint a strip of every colour you use, cut it in half, and put one half in a south-facing window and the other in a closed drawer. Compare them after six months and after a year.
That is a controlled experiment with a real control, and it settles the question for your paints in your climate better than any published table. It is the change-one-thing-at-a-time rung applied to time.
Date the strips and photograph them at the start, because memory for colour is very poor. The half kept in the dark is the whole point: without it, a slow fade in both halves is invisible.
Bahan untuk langkah ini:
Set Serbuk Pigmen Tanah1 keping
Kanvas pelukis (terenggang)1 kepingAlatan diperlukan:
Set berus pelukis
Pembaris4
4
Thin paint fades first
Thin paint fades first
A thin wash or a glaze has far less pigment per unit area than a solid layer, so destroying a given fraction of it changes the colour far more. The same pigment can look permanent in a thick passage and fade visibly where it was used thinly.
Watercolour is therefore the most vulnerable medium of all: thin films, no protective varnish, and traditionally full of lakes. That is why watercolours are shown under low light and stored in the dark, and why the ones that survive were painted with earths and mineral colours.
Which turns lightfastness into a design decision rather than a purchasing one. If a colour must be thin and must last, it has to be a mineral pigment — and if the only pigment with that hue is fugitive, the honest answer is to change the picture.
Bahan untuk langkah ini:
Set Serbuk Pigmen Tanah1 keping
Gam Arab1 kepingAlatan diperlukan:
Set berus pelukis
Kanta Pembesar Tukang EmasBahan
3- 1 kepingPemegang Tempat
- 1 kepingPemegang Tempat
- 1 kepingPemegang Tempat
Blueprint berkaitan
Blueprint ini berkongsi pengetahuan — teknik, bahan atau prinsip

Berbahaya
Making Lead White (Flake White) — The Dutch Stack Process for the Most Important Pigment in Oil Painting History
oleh Charlie
SENI
84
0
0
0
5
0

What Paint Is: Pigment, Binder, and the Ratio Between Them
oleh Mary
Kimia
11
0
0
0
0
0

One Reading Is Not a Measurement: Repeat It, and Look at the Spread
oleh Penny
Kejuruteraan
20
0
0
0
0
0
CC0 Domain Awam
Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.
Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.