Phosphor-Tin: Sponge Tin and Stick Phosphorus Layered in Charcoal and Heated in a Sealed Crucible (Berthold, US 658,230)
Phosphorus is hard to get into bronze without fire and fumes. Berthold packs sponge tin and sticks of phosphorus in layers of charcoal in a sealed crucible; as it heats, the tin melts and soaks up the phosphorus.
Result: phosphor-tin with about 10 % phosphorus, ready to add to molten copper.
Source: Berthold, US 658,230 (1900). Danger: white phosphorus is poisonous and catches fire in air. Picture drawn by Youblob.
Lanjutan
1 day
Kandungan berbahaya
Blueprint ini mengandungi prosedur berbahaya. Log masuk dan aktifkan kandungan berbahaya dalam tetapan akaun anda untuk melihat arahan langkah demi langkah.
Log masukBlueprint ini membuat
CC0 Domain Awam
Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.
Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.