Silver Oxide: Silver Nitrate Precipitated with Solution of Potassa (USP 1870)
Silver oxide is a heavy, dark brown powder, and heating it to about 250 °C leaves pure silver. Potash added to a silver nitrate solution throws it down, and washing leaves potassium nitrate behind in the water.
Source: US Pharmacopoeia 1870, as quoted in the US Dispensatory (1907), Argenti Oxidum. Not given here: the strength of the solution of potassa; ours: potassium hydroxide in distilled water. Silver nitrate stains and burns skin: gloves and goggles. Picture drawn by Youblob.
Pemula
1 day
Arahan
1
1
Dissolve 4 troy oz silver nitrate in half a pint of water
Dissolve 4 troy oz silver nitrate in half a pint of water
Dissolve 4 troy ounces of silver nitrate in half a pint of distilled water. Silver nitrate stains and burns skin: gloves and goggles.
Bahan untuk langkah ini:
Perak Nitrat4 troy oz
Air Suling0.5 pintAlatan diperlukan:
Neraca dua piring
Bikar Borosilikat
Rod Kaca Borosilikat
Sarung Tangan Nitril
Gogal Percikan Kimia2
2
Add solution of potassa while it still precipitates
Add solution of potassa while it still precipitates
Add solution of potassa, about a pint and a half or as much as needed, for as long as it still throws down a precipitate. Ours: potassium hydroxide dissolved in distilled water; the USP strength is not given here. Potash free of carbon dioxide keeps out silver carbonate.
Bahan untuk langkah ini:
Kalium hidroksida1 as required
Air Suling1.5 pintAlatan diperlukan:
Bikar Borosilikat
Rod Kaca Borosilikat
Sarung Tangan Nitril
Gogal Percikan Kimia3
3
Wash, dry and store in the dark
Wash, dry and store in the dark
Wash the precipitate again and again with water until the washings are almost tasteless. Dry it and keep it in a well-stoppered bottle away from light. Ours: filter paper, and a low oven, well below the 250 °C at which it breaks down to silver.
Alatan diperlukan:
Kertas Turas
Air Suling
Ketuhar pengeringan
Balang Kaca Gelap Bertutup KedapBahan
3- 4 troy ozPemegang Tempat
- 2 pintPemegang Tempat
- 1 as requiredPemegang Tempat
Alatan Diperlukan
9- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
Blueprint ini membuat
Blueprint berkaitan
Blueprint ini berkongsi pengetahuan — teknik, bahan atau prinsip
CC0 Domain Awam
Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.
Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.