Wire-Arc Spray Gun: Two Crossed Wires, a Vibrating Arc and an Air Blast (Schoop, US 1,133,508, 1915)
The first wire-arc metal sprayer. Two metal wires are pushed through iron tubes until their tips cross. Current through the wires also runs an electromagnet that pulls one tube back, so a small arc springs between the tips and melts them; a jet of air blows the molten metal off as a fine spray and puts the arc out, the magnet lets go, the wires touch again, and the cycle repeats very fast.
Result: a continuous spray of molten metal for coating a surface.
Source: M. U. Schoop, US 1,133,508 (1915). Unknown: the wire metals and sizes, the coil, the air pressure. Picture: the patent drawing.
Lanjutan
Unknown
Arahan
1
1
Make the feed tubes and rolls
Make the feed tubes and rolls
Make two feed tubes ending in nozzles, preferably of iron. For each, mount a pair of feed rolls in a frame to push a wire through the tube. Set the tubes at about 90° to each other so the wires cross as they come out, the nozzles only a few millimetres apart. Mount one tube on an elastic support so it can move a little. Not given: sizes, the roll drive (the air blast may drive a small turbine for it).
Bahan untuk langkah ini:
Tiub besi2 feed tubes
Logam tidak diketahui1 rolls, frames
Spring daun1 elastic supportAlatan diperlukan:
Mesin Pelarik Logam
Dimensi tidak diketahui2
2
Fit the electromagnet
Fit the electromagnet
Wind an electromagnet beside the springing tube, so the tube is its armature. Wire the coil into the same circuit as the two tubes and wires, positive to one tube and negative to the other. When current flows the magnet pulls the tube aside and draws its wire slightly back from the other. Ours: enamelled copper wire for the coil. Not given: the coil.
Bahan untuk langkah ini:
Dawai Kuprum Bersalut Enamel1 coil
Logam tidak diketahui1 magnet core
Dawai Tembaga1 circuit leadsAlatan diperlukan:
Set pemutar skru3
3
Fit the air blast
Fit the air blast
Aim a blast pipe at the point where the wires cross, either close to it or 20-30 mm away, whichever sprays best for the metal. Feed it with compressed air or another gas. Not given: the pressure.
Bahan untuk langkah ini:
Muncung udara1 keping
Hos angin1 kepingAlatan diperlukan:
Pemampat udara industri
Sepana boleh laras4
4
Spray
Spray
Load a wire of the coating metal in each tube and feed them until they touch. Switch on the current, generally 40 to 75 volts depending on the metal and wire thickness, and the air. The magnet pulls the wires apart, an arc melts their tips, the air blows the melt away as spray and snuffs the arc, the magnet releases, and the cycle repeats very rapidly. The positive wire burns faster, so feed it faster or use a thicker wire; match the feed to the melting. Hold the work in the spray. Without the vibration the arc flickers and the wires may weld together.
Alatan diperlukan:
Unit kuasa arus terus
Pemampat udara industri
Logam tidak diketahuiBahan
7- 2 feed tubesPemegang Tempat
- 1 magnet corePemegang Tempat
- 1 elastic supportPemegang Tempat
- Pemegang Tempat
- 1 circuit leadsPemegang Tempat
- 1 kepingPemegang Tempat
- 1 kepingPemegang Tempat
Alatan Diperlukan
7- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
Bahan Blueprint Bersambung
Blueprint ini membuat
CC0 Domain Awam
Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.
Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.