Wire Cutters: Diagonal Pliers Forged with Hardened V-Edged Jaws
Forge

Dicipta oleh

Forge

14. Oktober 2026NO
23
0
0
0
0

Wire Cutters: Diagonal Pliers Forged with Hardened V-Edged Jaws

Diagonal pliers cut wire by pressing two V-shaped edges into it until it splits, not by shearing like scissors. The edges sit at an angle to the joint rivet, which gives them their name, and the jaws must be hardened or steel wire dents them. Forge two halves from tool steel, rivet them, grind the edges and harden the jaws. The picture: the jaws and joint of a modern pair; its handles are dipped in plastic, ours are bare steel.
Lanjutan
Two days

Arahan

1

Forge the halves

Forge two mirror halves from tool steel: a short, thick jaw set at an angle, a flat boss for the joint, and a handle (our sizes: jaw 18 mm, handle 120 mm from the joint).

Bahan untuk langkah ini:

Bar keluli alat segi lapanBar keluli alat segi lapan0.3 kg
ArangArang2 as required

Alatan diperlukan:

Relau tukang besiRelau tukang besi
AndasAndas
Tukul kepala baji lintangTukul kepala baji lintang
Penyepit tukang besiPenyepit tukang besi
Sarung tangan kimpalanSarung tangan kimpalan
Cermin mata keselamatanCermin mata keselamatan
2

Anneal and fit the joint

Anneal both halves. File the bosses flat so they lap closely, drill them together and rivet them so the jaws close without play.

Bahan untuk langkah ini:

Rivet keluliRivet keluli1 keping

Alatan diperlukan:

Relau tukang besiRelau tukang besi
Kikir LogamKikir Logam
Gerimit tanganGerimit tangan
Ragum bangku beratRagum bangku berat
Tukul kepala baji lintangTukul kepala baji lintang
AndasAndas
3

Grind the edges

Grind each jaw to a symmetrical V so the two edges meet along their whole length when closed. Check against the light.

Alatan diperlukan:

Batu canai rodaBatu canai roda
Kikir LogamKikir Logam
4

Harden the jaws

Heat the jaws only to cherry red and quench in water. Polish them bright, then warm the joint and let the colour run to the edges; quench at straw (our temper).

Bahan untuk langkah ini:

AirAir10 liter

Alatan diperlukan:

Relau tukang besiRelau tukang besi
Baldi pelindapkejutanBaldi pelindapkejutan
Penyepit tukang besiPenyepit tukang besi
Sarung tangan kimpalanSarung tangan kimpalan
Cermin mata keselamatanCermin mata keselamatan
5

Hone and test

Hone the edges lightly on the stone and try them on soft copper wire first. A dent in the edge means the jaw is too soft.

Alatan diperlukan:

Batu asah grit 1000Batu asah grit 1000
6

Force at the edges

Memuatkan buku nota Jupyter…

Bahan

4
  • Pemegang Tempat
  • 2 as required
    Pemegang Tempat
  • 1 keping
    Pemegang Tempat
  • 10 liter
    Pemegang Tempat

Alatan Diperlukan

12

CC0 Domain Awam

Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.

Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.