Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Acetone

Philips' Ponjee and Verwijlen (US 4,639,382, 1987) made silver hold on acrylic by first dipping it in tannin dissolved in water mixed with an organic solvent; tannin in plain water gave no bond. This is their acetone solution: 45–90 % water, 10–55 % acetone by volume, 2.7–5.5 g tannin per litre, which gave full bonding in their cross-cut test. The sheet is then sensitised with weak stannous chloride and silvered by spraying the silver solution and the reducer together. The picture: our diagram.
Àárín
2 hours

Ìlànà

1

Dip in tannin solution for one minute

Make a solution of 2.7–5.5 g of tannic acid per litre in 45–90 % water and 10–55 % acetone by volume. Dip the acrylic sheet in it for one minute.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Pẹlẹbẹ AkrílíìkìPẹlẹbẹ Akrílíìkì1 ẹyọ

Àwọn irinṣẹ́ tí a nílò:

Tanikì ÁsídìTanikì Ásídì
AcetoneAcetone
Omi Àyọ́Omi Àyọ́
Àwo dígíÀwo dígí
Silinda òǹwọ̀nSilinda òǹwọ̀n
Òǹwọ̀n ìdọ́gbaÒǹwọ̀n ìdọ́gba
Àpótí eérú (tí ó ní ọ̀pá ìjáde)Àpótí eérú (tí ó ní ọ̀pá ìjáde)
Ìbọ̀wọ́ rọ́bàÌbọ̀wọ́ rọ́bà
2

Rinse with water

Rinse the sheet with water.

Àwọn irinṣẹ́ tí a nílò:

Omi Àyọ́Omi Àyọ́
Ìgò Fífọ̀Ìgò Fífọ̀
3

Spray with stannous chloride for 12 seconds

Spray the face to be silvered with a solution of 0.1 g stannous chloride and 0.1 ml concentrated hydrochloric acid per litre of water, for 12 seconds. Rinse off the excess with water.

Àwọn irinṣẹ́ tí a nílò:

Sitanọ́ọ̀sì KloraidiSitanọ́ọ̀sì Kloraidi
Hydrochloric acidHydrochloric acid
Omi Àyọ́Omi Àyọ́
Ìgò ìfọn omiÌgò ìfọn omi
Ìgò Fífọ̀Ìgò Fífọ̀
Gílásì Ààbò Fún Ìfọ́n Kẹ́míkàGílásì Ààbò Fún Ìfọ́n Kẹ́míkà
Ìbọ̀wọ́ rọ́bàÌbọ̀wọ́ rọ́bà
4

Spray silver and reducer together

Atomise two solutions onto the face at the same time: silver nitrate with ammonia in water, and formalin in water. The patent gives no strengths: as required. Ours: a twin-nozzle spray gun.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Silver NitrateSilver Nitrate1 as required

Àwọn irinṣẹ́ tí a nílò:

Omi amonia - 25-28 %Omi amonia - 25-28 %
Omi formaldehyde (formalin 37 %)Omi formaldehyde (formalin 37 %)
Omi Àyọ́Omi Àyọ́
Ìbọn Fífọ́n Ihò MéjìÌbọn Fífọ́n Ihò Méjì
Àpótí eérú (tí ó ní ọ̀pá ìjáde)Àpótí eérú (tí ó ní ọ̀pá ìjáde)
Gílásì Ààbò Fún Ìfọ́n Kẹ́míkàGílásì Ààbò Fún Ìfọ́n Kẹ́míkà
Ìbọ̀wọ́ rọ́bàÌbọ̀wọ́ rọ́bà

Àwọn ohun-èlò

2

Àwọn irinṣẹ́ tó nílò

16

Ìtọ́nisọ́nà yìí ń ṣe

Blueprint tó jọra

Àwọn blueprint wọ̀nyí pín ìmọ̀ — ọ̀nà, ohun-èlò tàbí ìlànà

CC0 Àgbègbè Gbogbogbò

Blueprint yìí ti jáde lábẹ́ CC0. O lè ṣe àdàkọ, yí padà, pín, àti lò láìsí ìyọ̀ǹda.

Ṣàtìlẹ́yìn Olùṣẹ́dá nípa rírà àwọn ọjà nipasẹ̀ Blueprint wọn Ẹ̀san Olùṣẹ́dá tí àwọn Olùtajà gbé kalẹ̀, tàbí ṣẹ̀dá àtúnṣe tuntun ti Blueprint yìí kí o sì fi sínú Blueprint rẹ gẹ́gẹ́ bí ìsopọ̀ láti pín owó-wíwọlé.

Ìfọ̀rọ̀wérọ̀

(0)

Wọlé láti dara pọ̀ mọ́ ìfọ̀rọ̀wérọ̀

Ń gbé àwọn ọ̀rọ̀ wọlé...