Carbon Resistance Ring: Laminated Paper Gelled with 15% Tung Oil, Graphite-Shellac Track

Mallory's quiet volume-control ring (US 2,144,925, 1939). Hard bases were noisy and soft paper ones changed with damp. Their answer: paper rings soaked in 15 % raw tung oil and baked, so the oil gels inside the paper. It shuts out moisture but stays soft and springy, and the wiper runs on it quietly. A graphite paint makes the track, silver paint the ends. The picture: the patent's drawing (Fig. 3).
Àárín
1 day

Ìlànà

1

Punch rings from three-ply paper

The base is three papers stuck into one sheet: litho paper at the back, newsprint in the middle, manila on the face that takes the track. Punch rings from it. Ours: a punch press with a ring die.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Bébà aláwọ̀ mẹ́ta tí a lẹ̀ pọ̀Bébà aláwọ̀ mẹ́ta tí a lẹ̀ pọ̀1 ẹyọ

Àwọn irinṣẹ́ tí a nílò:

Ẹ̀rọ ìtẹ̀ ìlu ihòẸ̀rọ ìtẹ̀ ìlu ihò
Dáì fún gígé òrùkaDáì fún gígé òrùka
Ìbọ̀wọ́ rọ́bàÌbọ̀wọ́ rọ́bà
2

Soak 1 hour in 15 % tung oil in naphtha

Soak the rings for about one hour in about 15 % raw tung oil in naphtha. Use raw oil, not heat-bodied or treated oil, so it can still gel.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Òróró tungÒróró tung15 parts

Àwọn irinṣẹ́ tí a nílò:

NaphthaNaphtha
Ago GílásìAgo Gílásì
Òǹwọ̀n ìdọ́gbaÒǹwọ̀n ìdọ́gba
Ohun ìrúwéOhun ìrúwé
Ìbòjú ìmí tí ó bo gbogbo ojúÌbòjú ìmí tí ó bo gbogbo ojú
Ìbọ̀wọ́ rọ́bàÌbọ̀wọ́ rọ́bà
3

Air-dry, then bake at 210–250 °C

Dry the rings in air for two hours or more, then bake 15 to 30 minutes at 210 to 250 °C. The oil gels in the paper's pores; the paper stays pliable.

Àwọn irinṣẹ́ tí a nílò:

Ààrò ìgbẹ̀Ààrò ìgbẹ̀
Ìwọ̀n Ooru ÀàròÌwọ̀n Ooru Ààrò
Ìbọ̀wọ́ Tí Ń Fara Da OoruÌbọ̀wọ́ Tí Ń Fara Da Ooru
4

Spray the graphite track

Spray on the resistance paint, for example graphite in a shellac binder. The patent gives no proportions. The track can be tapered in thickness, width or mix to shape the resistance curve.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Ẹ̀kù GraphiteẸ̀kù Graphite1 as required
Sẹ́làkìSẹ́làkì1 as required

Àwọn irinṣẹ́ tí a nílò:

Ìbọn ÌfúnpọnÌbọn Ìfúnpọn
Ẹ̀rọ ìfun afẹ́fẹ́Ẹ̀rọ ìfun afẹ́fẹ́
Ìbòjú ìmí tí ó bo gbogbo ojúÌbòjú ìmí tí ó bo gbogbo ojú
Ìbọ̀wọ́ rọ́bàÌbọ̀wọ́ rọ́bà
5

Paint silver ends, bake at 220 °C

Spray or paint the two end terminals with silver particles in shellac. Dry, then bake at about 220 °C to cure and harden the track. The slight warp from soaking flattens out again.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Kùn fàdákà tí ń gba iná mànàmánáKùn fàdákà tí ń gba iná mànàmáná1 as required

Àwọn irinṣẹ́ tí a nílò:

Ìbọn ÌfúnpọnÌbọn Ìfúnpọn
Ààrò ìgbẹ̀Ààrò ìgbẹ̀
Ìwọ̀n Ooru ÀàròÌwọ̀n Ooru Ààrò
Ìbọ̀wọ́ Tí Ń Fara Da OoruÌbọ̀wọ́ Tí Ń Fara Da Ooru

Àwọn ohun-èlò

5

Àwọn irinṣẹ́ tó nílò

13

Ìtọ́nisọ́nà yìí ń ṣe

CC0 Àgbègbè Gbogbogbò

Blueprint yìí ti jáde lábẹ́ CC0. O lè ṣe àdàkọ, yí padà, pín, àti lò láìsí ìyọ̀ǹda.

Ṣàtìlẹ́yìn Olùṣẹ́dá nípa rírà àwọn ọjà nipasẹ̀ Blueprint wọn Ẹ̀san Olùṣẹ́dá tí àwọn Olùtajà gbé kalẹ̀, tàbí ṣẹ̀dá àtúnṣe tuntun ti Blueprint yìí kí o sì fi sínú Blueprint rẹ gẹ́gẹ́ bí ìsopọ̀ láti pín owó-wíwọlé.

Ìfọ̀rọ̀wérọ̀

(0)

Wọlé láti dara pọ̀ mọ́ ìfọ̀rọ̀wérọ̀

Ń gbé àwọn ọ̀rọ̀ wọlé...