Teaspoon Forged from a Silver Bar (Payne 1914)
English
Arthur F. Payne · Public domain (1914)
Forge

Ṣẹ́dá nipasẹ̀

Forge

27. Oṣù Kẹwà 2026NO
24
0
0
0
0

Teaspoon Forged from a Silver Bar (Payne 1914)

A 6-inch silver teaspoon forged out of a small bar of silver, the way a blacksmith forges iron. Arthur Payne called it the hardest of his five spoon methods, but the cheapest, because almost no silver is wasted. Source: A. F. Payne, Art Metalwork with Inexpensive Equipment (1914), pp. 184–186; annealing from his chapter XI. Cutting the bar from sheet is ours. Picture: Payne's Fig. 158, teaspoons forged this way.
Ilọsíwájú
1 day

Ìlànà

1

Cut the silver bar

For a teaspoon 6 in long you need a piece of sterling silver 4 in long, ½ in wide and ⅛ in thick. Mark it out and saw it from sheet of that thickness (cutting from sheet is ours).

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

Abala Fàdákà Sítẹ́líìnìAbala Fàdákà Sítẹ́líìnì1 piece 4 × ½ × ⅛ in

Àwọn irinṣẹ́ tí a nílò:

Abẹ́rẹ́ Ìkọ ÌlàAbẹ́rẹ́ Ìkọ Ìlà
Ayùn Alágbẹ̀dẹ WúràAyùn Alágbẹ̀dẹ Wúrà
2

Forge out the bowl

Heat the bar until it is almost red-hot, hold it in tongs and forge the bowl out on the anvil. Silver forges more easily when it is nearly red, but never hammer it while it is red-hot: it will crack.

Àwọn irinṣẹ́ tí a nílò:

Ọ̀gọ̀ BunsenỌ̀gọ̀ Bunsen
Ẹ̀múẸ̀mú
Ìdí Alágbẹ̀dẹÌdí Alágbẹ̀dẹ
ÒòlùÒòlù
3

Work bowl, then shank and handle

Hammer the bowl until it is hard, then the shank and handle, so the whole spoon is hard before you anneal it again. That saves time.

Àwọn irinṣẹ́ tí a nílò:

Ìdí Alágbẹ̀dẹÌdí Alágbẹ̀dẹ
ÒòlùÒòlù
4

Anneal and repeat

To soften it, heat it to a dull red and plunge it into water, or let it cool. Then go on forging until the spoon is roughly to shape.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

OmiOmi1 as required

Àwọn irinṣẹ́ tí a nílò:

Ọ̀gọ̀ BunsenỌ̀gọ̀ Bunsen
Ẹ̀múẸ̀mú
Ohun èlò dígíOhun èlò dígí
5

Trim with shears and file

Trim the outline with the shears and file the edges smooth.

Àwọn irinṣẹ́ tí a nílò:

Ìkẹ́rẹ́ irin alágbáraÌkẹ́rẹ́ irin alágbára
Àwọn Ìfá (Ìfá Ọwọ́)Àwọn Ìfá (Ìfá Ọwọ́)
6

Polish out the file marks

Rub out all the scratches and file marks with emery cloth.

Àwọn irinṣẹ́ tí a nílò:

Aṣọ emeryAṣọ emery
7

Anneal to even the fire scale

Anneal the spoon thoroughly once more. Heated silver grows a thin white skin, the fire scale, and this brings it back over the spots where filing and polishing took it off, so the colour is even.

Àwọn ohun èlò fún ìgbésẹ̀ yìí:

OmiOmi1 as required

Àwọn irinṣẹ́ tí a nílò:

Ọ̀gọ̀ BunsenỌ̀gọ̀ Bunsen
Ẹ̀múẸ̀mú
Ohun èlò dígíOhun èlò dígí
8

Planish with smooth hammers

Planish the spoon on smooth tools with smooth, bright hammers. This makes it stiff again after the annealing.

Àwọn irinṣẹ́ tí a nílò:

Òòlù ìdánÒòlù ìdán
Ìdí Alágbẹ̀dẹÌdí Alágbẹ̀dẹ
Igi tí a gúnIgi tí a gún
9

Final polish with rouge

Polish it lightly with a soft cotton flannel and a little red rouge.

Àwọn irinṣẹ́ tí a nílò:

Aṣọ ìfọ́ ohun ọ̀ṣọ́Aṣọ ìfọ́ ohun ọ̀ṣọ́
Pupa ìdán alágbẹ̀dẹ wúràPupa ìdán alágbẹ̀dẹ wúrà

Àwọn ohun-èlò

2

Àwọn irinṣẹ́ tó nílò

14

Ìtọ́nisọ́nà yìí ń ṣe

CC0 Àgbègbè Gbogbogbò

Blueprint yìí ti jáde lábẹ́ CC0. O lè ṣe àdàkọ, yí padà, pín, àti lò láìsí ìyọ̀ǹda.

Ṣàtìlẹ́yìn Olùṣẹ́dá nípa rírà àwọn ọjà nipasẹ̀ Blueprint wọn Ẹ̀san Olùṣẹ́dá tí àwọn Olùtajà gbé kalẹ̀, tàbí ṣẹ̀dá àtúnṣe tuntun ti Blueprint yìí kí o sì fi sínú Blueprint rẹ gẹ́gẹ́ bí ìsopọ̀ láti pín owó-wíwọlé.

Ìfọ̀rọ̀wérọ̀

(0)

Wọlé láti dara pọ̀ mọ́ ìfọ̀rọ̀wérọ̀

Ń gbé àwọn ọ̀rọ̀ wọlé...