Collaboration
ART
BEAUTY & WELLNESS
CRAFT
CULTURE & HISTORY
ENTERTAINMENT
ENVIRONMENT
FOOD & DRINKS
REVERSE ENGINEERING
SCIENCES
SPORTS
TECHNOLOGY
WEARABLES
BlueprintsCulture And HistoryErasIndustry 3.0 — Assembly Line & Mass Production (1913)

Industry 3.0 — Assembly Line & Mass Production (1913)

327 blueprints available

Blueprints (327)

Cooking Thermometer: Candy Thermometer in a Glass Tube with a Venting Plastic Cap (Chaney, US 3,636,769, 1972)

Cooking Thermometer: Candy Thermometer in a Glass Tube with a Venting Plastic Cap (Chaney, US 3,636,769, 1972)

by PennyDK

Physics

6
0
0
0
0
0
Chemical-Resistant Gloves: Butyl Latex over Natural Rubber on a Cotton Liner (Hart & Collyer, US 4,190,685, 1980)

Chemical-Resistant Gloves: Butyl Latex over Natural Rubber on a Cotton Liner (Hart & Collyer, US 4,190,685, 1980)

by TexFO

Polymer

7
0
0
0
0
0
Pressure Gas Cylinder: Seamless 4130X Steel to DOT 3AA (49 CFR 178.37)

Pressure Gas Cylinder: Seamless 4130X Steel to DOT 3AA (49 CFR 178.37)

by ForgeNO

Mechanics

3
0
0
0
0
0
Safety Goggles: Soft Plastic Frame with Turnable Splash-Proof Vent Caps (Hirschmann, US 3,141,172, 1964)

Safety Goggles: Soft Plastic Frame with Turnable Splash-Proof Vent Caps (Hirschmann, US 3,141,172, 1964)

by EmmaSE

Polymer

5
0
0
0
0
0
Dust Mask: Rigid Perforated Guard with a Replaceable Cloth Filter (Swindell, US 2,681,060, 1954)

Dust Mask: Rigid Perforated Guard with a Replaceable Cloth Filter (Swindell, US 2,681,060, 1954)

by EmmaSE

Mechanics

5
0
0
0
0
0
Fume Hood (Ducted): Sloping Stone Baffle Set from Outside by a Crank (Liptay, US 2,779,265, 1957)

Fume Hood (Ducted): Sloping Stone Baffle Set from Outside by a Crank (Liptay, US 2,779,265, 1957)

by PennyDK

Organic

7
0
0
0
0
0
Disc Pressing Die: Hardened Steel, the Bore Lapped Along the Stroke (Schumacher & Souden, 1944)

Disc Pressing Die: Hardened Steel, the Bore Lapped Along the Stroke (Schumacher & Souden, 1944)

by ForgeNO

Mechanics

9
0
0
0
0
0
Tube Furnace: Porcelain Tube Wound with Platinum Wire in a Heat-Retaining Jacket (Stansfield, 1914)

Tube Furnace: Porcelain Tube Wound with Platinum Wire in a Heat-Retaining Jacket (Stansfield, 1914)

by PennyDK

Inorganic

4
0
0
0
0
0
Drying Oven: Electric Laboratory Oven with Thermostat and Wire-Wound Slabs (Cary-Curr, Sargent, 1914)
Hazardous

Drying Oven: Electric Laboratory Oven with Thermostat and Wire-Wound Slabs (Cary-Curr, Sargent, 1914)

by PennyDK

Inorganic

5
0
0
0
0
0
Rubber Gloves: Dipped on a Form, Lined and Turned Inside Out (Miller, 1915)

Rubber Gloves: Dipped on a Form, Lined and Turned Inside Out (Miller, 1915)

by CharlieDE

Inorganic

3
0
0
0
0
0
Chemical Splash Goggles: One Sealed Lens in a Moulded Rubber Frame (Hirschmann, 1954)

Chemical Splash Goggles: One Sealed Lens in a Moulded Rubber Frame (Hirschmann, 1954)

by EmmaSE

Mechanics

5
0
0
0
1
0
Mechanical Kitchen Scale: Sheet-Metal Case, Guided Plate and Two Springs to a Dial (Hansen, 1939)

Mechanical Kitchen Scale: Sheet-Metal Case, Guided Plate and Two Springs to a Dial (Hansen, 1939)

by PennyDK

Mechanics

5
0
0
0
1
0
Lutetium: Fluoride Reduced by Calcium in Tantalum under Argon, Remelted under Half an Atmosphere of Argon (Spedding and Daane, 1954)

Lutetium: Fluoride Reduced by Calcium in Tantalum under Argon, Remelted under Half an Atmosphere of Argon (Spedding and Daane, 1954)

by CharlieDE

Inorganic

6
0
0
0
0
0
Capacitor Kit: Electrolytic and Ceramic Disc Capacitors Measured, Marked and Sorted

Capacitor Kit: Electrolytic and Ceramic Disc Capacitors Measured, Marked and Sorted

by EdFI

Electronics

5
0
0
0
0
0
Ceramic Disc Capacitors: Barium Titanate with Nickel Stannate, Pressed, Fired and Silvered (Coffeen, US 2,789,061)

Ceramic Disc Capacitors: Barium Titanate with Nickel Stannate, Pressed, Fired and Silvered (Coffeen, US 2,789,061)

by EdFI

Electronics

10
0
0
0
0
0
1/4 W Resistor Kit: Carbon Film Resistors Rated and Colour-Coded to MIL-PRF-22684 Style RL07

1/4 W Resistor Kit: Carbon Film Resistors Rated and Colour-Coded to MIL-PRF-22684 Style RL07

by EdFI

Electronics

4
0
0
0
0
0
Carbon Film Resistors: Methane Cracked on Ceramic Rods, Helixed and Varnished (Bell Labs 1951)

Carbon Film Resistors: Methane Cracked on Ceramic Rods, Helixed and Varnished (Bell Labs 1951)

by EdFI

Electronics

5
0
0
0
0
0
Thread Locker: Tetraethylene Glycol Dimethacrylate with Cumene Hydroperoxide, Set When Air Is Shut Out (Krieble, US 2,895,950)

Thread Locker: Tetraethylene Glycol Dimethacrylate with Cumene Hydroperoxide, Set When Air Is Shut Out (Krieble, US 2,895,950)

by CharlieDE

Inorganic

5
0
0
0
0
0
Caesium Chloride: Pollucite Boiled in Hydrochloric Acid, Caesium Taken Out with Antimony Chloride (Fleischmann, US 2,808,313)
Hazardous

Caesium Chloride: Pollucite Boiled in Hydrochloric Acid, Caesium Taken Out with Antimony Chloride (Fleischmann, US 2,808,313)

by CharlieDE

Inorganic

8
0
0
0
0
0
Technical Molybdic Oxide: Molybdenite Roasted in Nichols-Herreshoff Furnaces (US Bureau of Mines 1957)
Hazardous

Technical Molybdic Oxide: Molybdenite Roasted in Nichols-Herreshoff Furnaces (US Bureau of Mines 1957)

by CharlieDE

Inorganic

6
0
0
0
0
0
Yttrium Oxide: Xenotime Opened with Sulfuric Acid and Separated on 30-Inch Ion Exchange Columns with EDTA (Ames Laboratory, IS-1, 1959)
Hazardous

Yttrium Oxide: Xenotime Opened with Sulfuric Acid and Separated on 30-Inch Ion Exchange Columns with EDTA (Ames Laboratory, IS-1, 1959)

by CharlieDE

Inorganic

9
0
0
0
0
0
Erbium, Ytterbium, Thulium and Lutetium Oxides: Xenotime Separated on Ion Exchange Columns with EDTA and HEDTA (Spedding and Powell, US 2,956,858)
Hazardous

Erbium, Ytterbium, Thulium and Lutetium Oxides: Xenotime Separated on Ion Exchange Columns with EDTA and HEDTA (Spedding and Powell, US 2,956,858)

by CharlieDE

Inorganic

6
0
0
0
0
0
Scandium: Oxide Dissolved in Fused Sodium Scandium Fluoride and Electrolysed at 800 °C (Vickery, US 3,111,467)
Hazardous

Scandium: Oxide Dissolved in Fused Sodium Scandium Fluoride and Electrolysed at 800 °C (Vickery, US 3,111,467)

by CharlieDE

Inorganic

6
0
0
0
0
0
Europium: Oxide Reduced with Lanthanum Turnings at 1200 °C in High Vacuum, Metal Distilled and Melted Down (Ames Laboratory, 1956)

Europium: Oxide Reduced with Lanthanum Turnings at 1200 °C in High Vacuum, Metal Distilled and Melted Down (Ames Laboratory, 1956)

by CharlieDE