Annealing Oven: a Firebrick Chamber over a Firebox
Bubbles

Nilikha ni

Bubbles

14. Oktubre 2026IT
10
0
0
0
0

Annealing Oven: a Firebrick Chamber over a Firebox

Annealing is holding work hot and letting it cool slowly so it loses its stresses or softens. Glass is held at about 454–482 °C for most kinds, then cooled slowly; metal is often left to cool in the oven with the fire out. Build a firebrick chamber over a small firebox, with a door, a damper and a pyrometer, so it can be held at heat and then shut up to cool. The picture: putting bottles into the annealing oven at a glass works, 1908 (Lewis Hine).
Katamtaman
Two days, then drying

Mga Tagubilin

1

Lay the firebox

On a level base, lay firebricks in refractory mortar for a small firebox with an opening for fuel and air.

Mga materyales para sa hakbang na ito:

Ladrilyong Matibay sa ApoyLadrilyong Matibay sa Apoy40 piraso
Argamasa ng luwad na matibay sa apoyArgamasa ng luwad na matibay sa apoy10 kg

Mga kailangang kasangkapan:

Dulos ng kanteroDulos ng kantero
Antas na May BurbuhaAntas na May Burbuha
2

Grate and chamber

Forge iron bars to lay across the top of the firebox as a floor with gaps for the heat, and build the chamber walls on it, leaving a flue hole in the roof.

Mga materyales para sa hakbang na ito:

Baras na pandayang bakalBaras na pandayang bakal4 piraso
Ladrilyong Matibay sa ApoyLadrilyong Matibay sa Apoy30 piraso
Argamasa ng luwad na matibay sa apoyArgamasa ng luwad na matibay sa apoy10 kg

Mga kailangang kasangkapan:

Pandayan ng pandayPandayan ng panday
PalihanPalihan
Martilyong pahalang ang tulisMartilyong pahalang ang tulis
Dulos ng kanteroDulos ng kantero
3

Door, damper and pyrometer

Fit an iron-sheet door lined with brick and a sliding sheet damper over the flue. Set the pyrometer through the side wall into the chamber.

Mga materyales para sa hakbang na ito:

Lata ng bakal (pinukpok)Lata ng bakal (pinukpok)2 piraso

Mga kailangang kasangkapan:

Martilyong pahalang ang tulisMartilyong pahalang ang tulis
PirometroPirometro
4

Dry and first firing

Let the mortar dry for several days, then fire gently with charcoal and raise the heat slowly. Practise holding the chamber at the heat you need, and shutting door, damper and firebox to cool it down slowly.

Mga materyales para sa hakbang na ito:

UlingUling10 as required

Mga kailangang kasangkapan:

PirometroPirometro
Guwantes na Matibay sa InitGuwantes na Matibay sa Init
5

Bricks for the oven

Naglo-load ng Jupyter notebook…

Mga Materyales

5

Mga Kinakailangang Kasangkapan

7

Ang blueprint na ito ay gumagawa ng

Kaugnay na Blueprint

Ang mga blueprint na ito ay nagbabahagi ng kaalaman — mga teknik, materyales, o prinsipyo

CC0 Pampublikong Domain

Ang blueprint na ito ay inilabas sa ilalim ng CC0. Malaya kang kumopya, magbago, mamahagi, at gumamit nang walang pahintulot.

Suportahan ang Maker sa pamamagitan ng pagbili ng mga produkto sa kanilang Blueprint Komisyon ng Maker itinakda ng mga Vendor, o lumikha ng bagong bersyon ng Blueprint na ito at isama bilang koneksyon sa iyong Blueprint upang ibahagi ang kita.

Talakayan

(0)

Mag-login upang sumali sa talakayan

Naglo-load ng mga komento...