Dysprosium: Oxide Reduced with Lanthanum Turnings at 1650 °C in High Vacuum, Metal Distilled Off (Sanden, Ames 1973)
Lanthanum holds oxygen more tightly than dysprosium does and is much less volatile. Heated together in a tantalum boiler under high vacuum, lanthanum takes the oxygen and dysprosium vapour rises through baffles onto a condenser, leaving lanthanum oxide behind.
Result: 125-155 g of dysprosium per run, 56-81 % yield.
Source: B. L. Sanden, A study of the reduction of dysprosium oxide with lanthanum (Iowa State University / Ames Laboratory, 1973), pp. 12-27. Work at 1650 °C in high vacuum; hot hydrochloric acid for cleaning. Picture drawn by Youblob.
Abantado
1 week
Mapanganib na nilalaman
Ang blueprint na ito ay naglalaman ng mga mapanganib na proseso. Mag-log in at i-enable ang mapanganib na nilalaman sa iyong account settings upang makita ang step-by-step na mga tagubilin.
Mag-sign inAng blueprint na ito ay gumagawa ng
Kaugnay na Blueprint
Ang mga blueprint na ito ay nagbabahagi ng kaalaman — mga teknik, materyales, o prinsipyo
CC0 Pampublikong Domain
Ang blueprint na ito ay inilabas sa ilalim ng CC0. Malaya kang kumopya, magbago, mamahagi, at gumamit nang walang pahintulot.
Suportahan ang Maker sa pamamagitan ng pagbili ng mga produkto sa kanilang Blueprint Komisyon ng Maker itinakda ng mga Vendor, o lumikha ng bagong bersyon ng Blueprint na ito at isama bilang koneksyon sa iyong Blueprint upang ibahagi ang kita.