Semi-Cured Phenolic Sheet: Paper Dipped in Phenol Resin and Part-Cured at 120-130 °C (Lucas, Western Electric, US 1,470,990)
Charlie

Nilikha ni

Charlie

31. Oktubre 2026DE
8
0
0
0
0

Semi-Cured Phenolic Sheet: Paper Dipped in Phenol Resin and Part-Cured at 120-130 °C (Lucas, Western Electric, US 1,470,990)

Paper soaked in phenol resin is dried, then cured only part of the way, so the resin is stiff but not yet hard. Lucas did this before the final hot press so the press would not squeeze the resin out of the fibres. Result: a dry, partly cured phenolic sheet that a later coat of phenolic resin can still bond into. Source: Lucas, US 1,470,990 (Western Electric, 1923). Stopping before his final hot press is ours. Not given: the solvent in his resin, paper grade, mercerising strengths. Picture drawn by Youblob.
Katamtaman
1 hour

Mga Tagubilin

1

Dip the paper in phenol resin

Run the paper through a bath of phenol resin of specific gravity about 0.970: about 2 minutes for plain paper, 1 minute or less if mercerised first. Ours: Liquid Bakelite as the resin; Lucas does not say how it was thinned.

Mga materyales para sa hakbang na ito:

PapelPapel1 as required
Likidong Bakelite (produktong kondensasyon ng phenol at formaldehyde)Likidong Bakelite (produktong kondensasyon ng phenol at formaldehyde)1 as required

Mga kailangang kasangkapan:

Linya ng pagbababad ng prepregLinya ng pagbababad ng prepreg
HydrometerHydrometer
2

Optional: mercerise the paper first

For faster, fuller soaking, first pass the paper through caustic soda, squeeze, wash in water, neutralise in an acid, wash again and dry. Strengths and the acid: not given.

Mga kailangang kasangkapan:

Lihiya (sodium hydroxide)Lihiya (sodium hydroxide)
Linya ng pagbababad ng prepregLinya ng pagbababad ng prepreg
3

Dry at about 90 °C

Dry the soaked paper in an oven at about 90 °C, just long enough to dry it.

Mga kailangang kasangkapan:

Hurnong pantuyoHurnong pantuyo
4

Part-cure at 120-130 °C

Pass the dry paper through a curing oven at 120-130 °C for about 10 minutes (Lucas's description; his claim 4 says 125 °C for about 10 seconds). The resin sets as stiff as the fibres, but does not harden through.

Mga kailangang kasangkapan:

Hurnong pampatigas ng patongHurnong pampatigas ng patong
5

Dip again for 10-15 seconds and dry

Dip the part-cured paper in phenol resin again for 10-15 seconds, then dry at about 90 °C until it can be wound on a reel. Stop here: the sheet is semi-cured. Lucas's next step, stacking and hot pressing, cures it fully.

Mga materyales para sa hakbang na ito:

Likidong Bakelite (produktong kondensasyon ng phenol at formaldehyde)Likidong Bakelite (produktong kondensasyon ng phenol at formaldehyde)1 as required

Mga kailangang kasangkapan:

Linya ng pagbababad ng prepregLinya ng pagbababad ng prepreg
Hurnong pantuyoHurnong pantuyo

Mga Materyales

2

Mga Kinakailangang Kasangkapan

5

Kaugnay na Blueprint

Ang mga blueprint na ito ay nagbabahagi ng kaalaman — mga teknik, materyales, o prinsipyo

CC0 Pampublikong Domain

Ang blueprint na ito ay inilabas sa ilalim ng CC0. Malaya kang kumopya, magbago, mamahagi, at gumamit nang walang pahintulot.

Suportahan ang Maker sa pamamagitan ng pagbili ng mga produkto sa kanilang Blueprint Komisyon ng Maker itinakda ng mga Vendor, o lumikha ng bagong bersyon ng Blueprint na ito at isama bilang koneksyon sa iyong Blueprint upang ibahagi ang kita.

Talakayan

(0)

Mag-login upang sumali sa talakayan

Naglo-load ng mga komento...