Silicon: Silica Heated with Magnesium Powder under Magnesia, Acid-Washed (Vigouroux, Thorpe 1912)
Magnesium burns the oxygen out of silica; extra magnesia keeps the reaction from running wild. A run of acids then dissolves everything but the silicon.
Result: amorphous silicon, a maroon powder with only 0.4–1 % impurity.
Source: Thorpe, Dictionary of Applied Chemistry vol. 4 (1912), p. 669, after Vigouroux (Compt. rend. 1895, 120, 94, 1161). Not given: amount of magnesia, temperature and vessel. Picture drawn by Youblob.
Abantado
2 days
Mapanganib na nilalaman
Ang blueprint na ito ay naglalaman ng mga mapanganib na proseso. Mag-log in at i-enable ang mapanganib na nilalaman sa iyong account settings upang makita ang step-by-step na mga tagubilin.
Mag-sign inAng blueprint na ito ay gumagawa ng
CC0 Pampublikong Domain
Ang blueprint na ito ay inilabas sa ilalim ng CC0. Malaya kang kumopya, magbago, mamahagi, at gumamit nang walang pahintulot.
Suportahan ang Maker sa pamamagitan ng pagbili ng mga produkto sa kanilang Blueprint Komisyon ng Maker itinakda ng mga Vendor, o lumikha ng bagong bersyon ng Blueprint na ito at isama bilang koneksyon sa iyong Blueprint upang ibahagi ang kita.