Stone Flat Chisel: the Marble Lettering Tool, Drawn Very Thin (Holford, 1907)
Forge

Nilikha ni

Forge

5. Nobyembre 2026NO
12
0
0
0
0

Stone Flat Chisel: the Marble Lettering Tool, Drawn Very Thin (Holford, 1907)

A flat chisel for cutting letters in marble. Frederick Holford's 20th Century Toolsmith (1907) makes marble tools like granite tools, from 7/8-inch octagon steel, but tempers them a little harder, to a very light straw. The lettering tool is drawn out very thin (his Fig. 69); because of that thinness it must be heated with great care, and the last few blows when dressing it are struck on the flat side only, at a very low heat. He gives no edge width, length or carbon content; those are unknown here. Source: F. J. Holford, The 20th Century Toolsmith and Steelworker (1907), p. 130, pp. 122-123 and p. 21 (the hardening bath). Picture: his Fig. 69.
Katamtaman
An hour

Mga Tagubilin

1

Read Holford

"Lettering tools are drawn out very thin, as Fig. 69, but owing to the thinness be very careful when heating, and make sure when dressing to always strike the last few blows on the flat side only, when at a very low heat."
2

Draw out the edge

Forge 7/8-inch octagon steel down to a straight edge, drawn out very thin (Fig. 69). Heat with great care because of the thinness. Strike the last few blows on the flat side only, at a very low heat. Straighten the edge with a very coarse file after hammering. Edge width and length are not given (unknown).

Mga materyales para sa hakbang na ito:

Oktagonal na barang tool steelOktagonal na barang tool steel1 bar

Mga kailangang kasangkapan:

PandayanPandayan
PalihanPalihan
Martilyo ng pandayMartilyo ng panday
Sipit ng pandaySipit ng panday
Kikil na Pang-metalKikil na Pang-metal
Hindi alam na sukatHindi alam na sukat
3

Harden and temper

Heat no farther back than 1/2 inch, taking care not to overheat the thin edge. Dip at least an inch deep into the hardening bath (p. 21: clean water, best a brine with as much salt as it will dissolve, large and cold) so the temper runs back slowly, and stop it at a very light straw, the marble temper.

Mga kailangang kasangkapan:

PandayanPandayan
Sipit ng pandaySipit ng panday
Puspos na solusyon ng asinPuspos na solusyon ng asin
Guwantes na Matibay sa InitGuwantes na Matibay sa Init
4

History and honest limits

Holford sets lettering tools apart from the tooth and plain chisels used to dress marble, which "are not drawn out so thin"; the teeth of tooth chisels are filed in after hammering (his Fig. 70). Edge width, length and the carbon of the steel are not given; an octagonal tool steel bar stands for the 7/8-inch octagon steel.

Mga Materyales

1

Mga Kinakailangang Kasangkapan

8

Ang blueprint na ito ay gumagawa ng

CC0 Pampublikong Domain

Ang blueprint na ito ay inilabas sa ilalim ng CC0. Malaya kang kumopya, magbago, mamahagi, at gumamit nang walang pahintulot.

Suportahan ang Maker sa pamamagitan ng pagbili ng mga produkto sa kanilang Blueprint Komisyon ng Maker itinakda ng mga Vendor, o lumikha ng bagong bersyon ng Blueprint na ito at isama bilang koneksyon sa iyong Blueprint upang ibahagi ang kita.

Talakayan

(0)

Mag-login upang sumali sa talakayan

Naglo-load ng mga komento...