Reading a Failed Print: The Fault Names Itself If You Look
A failed print is evidence. Where it went wrong, what the surface looks like, and at which layer it stopped all point at a cause — and there are only about a dozen causes.
The useful discipline is to look BEFORE changing anything. A print that failed halfway up failed for a different reason than one that never stuck, and a print with holes in the top surface has a different problem again from one that is stringy all over.
Then change ONE setting and print again. Changing four settings because a forum post listed four possibilities means that when it works you have learned nothing, and the next failure starts from zero.
درمیانہ
3 hours
ہدایات
1
1
Failures at the plate
Failures at the plate
NOTHING STUCK: nozzle too high, plate dirty, or plate cold. Check the first-layer rung's three tests in that order.
CORNERS LIFTED, rest fine: warping. Material, enclosure, draughts and corner radius — the warping rung.
PART CAME OFF PARTWAY UP: adhesion was marginal from the start and the growing part's shrinkage finally won. That is a warping failure presenting late, not an adhesion failure, and more glue will not fix it.
اس مرحلے کے لیے مواد:
تھری ڈی پرنٹنگ فلامنٹ (PLA)1 ٹکڑادرکار اوزار:
تار والا 3D پرنٹر (FDM)
تھری ڈی چھپائی اتارنے کی کھرپی سیٹ
مکبر لوپ2
2
Failures in the plastic
Failures in the plastic
STRINGS between parts: the nozzle is oozing while travelling. Too hot, or too little retraction, or wet filament — and wet filament is the one people check last and should check first if the filament has been open a while.
GAPS BETWEEN LINES and a weak, translucent part: under-extrusion. A partial blockage, a worn or slipping extruder gear, or the flow rate set too low.
BLOBS AND RIDGES, dimensions too large: over-extrusion. Flow too high, or the filament diameter in the slicer not matching what is actually loaded — a 1.75 mm setting on 1.70 mm filament is a few percent of error that shows on every wall.
اس مرحلے کے لیے مواد:
تھری ڈی پرنٹنگ فلامنٹ (PLA)1 ٹکڑادرکار اوزار:
مکبر لوپ
ڈیجیٹل ورنیئر کیلیپر ۶ انچ
فلامنٹ ڈرائر
تھری ڈی پرنٹر نوزل سیٹ3
3
Failures in the geometry
Failures in the geometry
SAGGING UNDERSIDES: an overhang past what the machine can do. The overhang rung's table says whether it was ever going to work at that layer height.
A LAYER SHIFT — everything above a certain height offset sideways — is mechanical, not a slicing problem. The nozzle hit something, a belt slipped, or a motor lost steps because it was moving too fast.
SPLITTING ALONG A LAYER after the print is finished: layer adhesion. Print hotter, slow down, reduce the fan, or re-orient — and if the part is loaded across its layers, re-orienting is the answer the other three are compensating for.
اس مرحلے کے لیے مواد:
تھری ڈی پرنٹنگ فلامنٹ (PLA)1 ٹکڑا
ABS فلامنٹ1 ٹکڑادرکار اوزار:
مکبر لوپ
تار والا 3D پرنٹر (FDM)
تھری ڈی پرنٹر اوزار کٹ4
4
Keep the failures, and keep a log
Keep the failures, and keep a log
Photograph the failure before throwing it away, and write down what the settings were. A drawer of labelled failures is a diagnostic reference that gets better every time something goes wrong.
Log every print that mattered: filament, temperature, speed, layer height, what came out. Filament varies between spools of the same brand, and a note saying "this spool needs 5 degrees hotter" saves the next three prints.
That is the notebook rung again, and it is the habit that separates a printer that works reliably from one that is a lottery. The settings that work for your machine are discoverable, and they are only discoverable by writing them down.
درکار اوزار:
ڈیسک ٹاپ کمپیوٹر
ڈیجیٹل ورنیئر کیلیپر ۶ انچمواد
2- پلیس ہولڈر
- 1 ٹکڑاپلیس ہولڈر
درکار اوزار
8- پلیس ہولڈر
- پلیس ہولڈر
- پلیس ہولڈر
- پلیس ہولڈر
- فلامنٹ ڈرائر10% کمیشنپلیس ہولڈر
- پلیس ہولڈر
- تھری ڈی پرنٹر اوزار کٹ10% کمیشنپلیس ہولڈر
- پلیس ہولڈر
متعلقہ بلیو پرنٹ
یہ بلیو پرنٹ علم بانٹتے ہیں — تکنیک، مواد یا اصول

The First Layer Decides Everything Above It
3DBonanza کی طرف سے
اضافی مصنوعات سازی
25
0
0
0
0
0

Overhangs, Bridges and Support: What the Machine Can Print Over Thin Air
3DBonanza کی طرف سے
اضافی مصنوعات سازی
19
0
0
0
0
0

Change One Thing at a Time: Grow the Control, and the Confounded Jar Too
Penny کی طرف سے
تجزیاتی
13
0
0
0
0
0
CC0 پبلک ڈومین
یہ بلیو پرنٹ CC0 کے تحت جاری کیا گیا ہے۔ آپ اجازت لیے بغیر اس کام کو نقل، ترمیم، تقسیم اور کسی بھی مقصد کے لیے استعمال کرنے کے لیے آزاد ہیں۔
میکر کی حمایت کریں ان کے بلیو پرنٹ کے ذریعے پروڈکٹس خرید کر جہاں وہ میکر کمیشن وینڈرز کی طرف سے مقرر، کماتے ہیں، یا اس بلیو پرنٹ کی نئی تکرار بنائیں اور آمدنی شیئر کرنے کے لیے اسے اپنے بلیو پرنٹ میں کنکشن کے طور پر شامل کریں۔