Bonded Wire Strain Gauge on Paper: Simmons, 1942
Edward E. Simmons, Jr. of Pasadena patented the bonded wire strain gauge in 1942, US 2,292,549 (filed 1940). A very fine resistance wire is cemented to a member along its entire length, so it stretches and shortens exactly with the surface and its electrical resistance follows the strain. His preferred form: Constantan or Advance wire, about 0.003 inch, wound back and forth on a thin paper, set in Glyptal, then cemented to the member and calibrated.
Zaawansowany
Workshop process
Instrukcje
1
1
Wind the filament on thin paper
Wind the filament on thin paper
Use a fine resistance wire such as Constantan or Advance (a copper-nickel alloy, about 45 % nickel and 55 % copper); Simmons used No. 40 gauge, about 0.0031 inch. Wind it back and forth across a thin paper in parallel lengths whose alternate ends are joined, the strands very close together but not touching. A winding jig keeps the filament slightly taut.
Materiały do tego kroku:
Drut konstantanowy1 as required
Papier1 arkuszPotrzebne narzędzia:
Przyrząd do nawijania
Nożyczki2
2
Set it in Glyptal
Set it in Glyptal
Cover the wound filament with Glyptal and let it dry and harden thoroughly. Filament and paper now form one gauge unit, the filament lying in the plane of the paper surface.
Materiały do tego kroku:
Żywica alkidowa Glyptal1 as requiredPotrzebne narzędzia:
Cienkie pędzle
Piec do suszenia3
3
Cement it to the member
Cement it to the member
Put Glyptal on the surface of the member and wrap the gauge unit on with the strands running in the direction of the strain to be measured, the paper outside. The small amount of Glyptal on the surface insulates the filament from the member. Hold filament and paper in place by wrapping them with thread, then dry and harden the Glyptal thoroughly.
Materiały do tego kroku:
Żywica alkidowa Glyptal1 as required
Nić bawełniana1 as requiredPotrzebne narzędzia:
Cienkie pędzle
Piec do suszenia
Nożyczki4
4
Calibrate it
Calibrate it
Load the member progressively in a materials testing machine and note the change in the filament's resistance at each load, measured on a Wheatstone bridge in which the filament is one arm. For very fast loads, as in impact tests, an oscillograph takes the place of the galvanometer.
Potrzebne narzędzia:
Maszyna wytrzymałościowa
Mostek Wheatstone'a
Galwanometr analogowy5
5
Bonding area and signal size
Bonding area and signal size
Wczytywanie notatnika Jupyter…
Materiały
4- 1 as requiredZastępnik
- 1 arkuszZastępnik
- 1 as requiredZastępnik
- 1 as requiredZastępnik
Wymagane narzędzia
7- Zastępnik
- Zastępnik
- Zastępnik
- Zastępnik
- Zastępnik
- Zastępnik
- Zastępnik
Według tego planu powstaje
Powiązane blueprinty
Te blueprinty dzielą się wiedzą — technikami, materiałami lub zasadami
CC0 Domena publiczna
Ten plan jest udostępniany na licencji CC0. Możesz go swobodnie kopiować, modyfikować, rozpowszechniać i wykorzystywać do dowolnych celów, bez konieczności uzyskiwania zgody.
Wesprzyj Makera kupując produkty przez jego plan, za co zarabia Prowizja Makera ustalony przez sprzedawców, lub stwórz nową iterację tego planu i dołącz go jako połączenie w swoim własnym planie, aby dzielić się przychodami.