Cupola Furnace: the Common Foundry Cupola with a Drop Bottom (Bolland, 1893)
The founder's 'common cupola': an upright steel shell lined with firebrick, standing on four columns over a drop bottom, with a wind-box round it feeding the tuyeres and a charging door high up. Coke and pig iron go in at the top in layers; blast at the tuyeres melts the iron, which runs out at the spout.
Variable: the inside diameter, 24 to 84 in, which sets height, tuyeres, blower and charges. Fig. 9's 36 in cupola is 12 ft to the charging hole and takes 840 lb coke and 2520 lb iron on the bed, then 302 lb coke and 2718 lb iron per charge.
Source: S. Bolland, The Iron Founder Supplement (1893), pp. 34-54. Unknown: shell plate and brick sizes. Picture: Fig. 9 of the book.
Ekspert
Unknown
Instrukcje
1
1
Size the cupola
Size the cupola
Choose the inside diameter from the iron needed per hour: 10 tons in two hours (about 10,760 lb an hour) needs 48 in; 6 tons, 40 in. Make it tall enough that the gas burns before it escapes: a 50 in cupola is 14 ft from the base to the bottom of the charging hole, Fig. 9's 36 in one 12 ft. Above 60 in, keep 60 in at the tuyeres and widen above them, since the blast cannot reach the middle of a wider stock.
Potrzebne narzędzia:
Nieznane wymiary2
2
Build the shell, columns and drop bottom
Build the shell, columns and drop bottom
Build a steel shell with a charging hole and door, standing on four columns. Close the bottom with swing doors on a central prop, so the whole contents can be dropped at the end of a heat. Put a slag hole a little below the tuyeres and a spout at the bottom. Ours: mild steel plate, iron castings for the bottom doors. Not given: plate thickness.
Materiały do tego kroku:
Blacha gruba ze stali niskowęglowej1 shell, charging door
Odlewy żeliwne1 drop-bottom doors
Nieznany metal1 columns, prop, spoutPotrzebne narzędzia:
Spawarka łukowa
Nieznane wymiary3
3
Fit the tuyeres and wind-box
Fit the tuyeres and wind-box
Ring the cupola with a wind-box feeding the tuyeres, with a main blast pipe sized from the table (good for runs up to 100 ft). Tuyere area grows with the diameter: a 24 in cupola needs the area of 1 1/2 round 6 in tuyeres (or two flat ones 10 1/2 x 2 in), a 60 in about 13 1/2 (or eight flat 16 1/2 x 3 in), an 84 in 31 (or sixteen flat 16 x 3 1/2 in). Never reduce the tuyere area. A 42 in cupola takes a No. 3 Root blower and a 6 h.p. engine.
Materiały do tego kroku:
Blacha gruba ze stali niskowęglowej1 wind-box
Nieznany metal1 tuyeres, blast pipePotrzebne narzędzia:
Spawarka łukowa
Dmuchawa4
4
Line it with firebrick
Line it with firebrick
Line the shell with firebrick, every brick rubbed well down on the next and fitting the shell closely, set in mortar of the same nature as the bricks. A good lining lasts one to two years if the melter mends it each morning with thin coats of daubing, keeping its first shape. Ours: fireclay bricks and refractory clay mortar.
Materiały do tego kroku:
Cegły szamotowe1 lining
Zaprawa z gliny ogniotrwałej1 setting and daubingPotrzebne narzędzia:
Kielnia5
5
Make the bed and melt
Make the bed and melt
Ram a sand bottom so it lies about 10 in below the tuyeres. Lay the fuel bed, about 22 in of coke above the tuyeres (840 lb in Fig. 9's 36 in cupola), and the first iron (2520 lb), then alternate charges of coke and iron (302 lb and 2718 lb). Blow: about 30,000 cubic feet of air melts a ton of iron. On long heats flux with white marble chips and draw the slag off at the slag hole. At the end, drop the bottom.
Potrzebne narzędzia:
Piasek
Koks hutniczy
Gąski surówki żelaza
DmuchawaMateriały
5- 1 wind-boxZastępnik
- 1 drop-bottom doorsZastępnik
- 1 tuyeres, blast pipeZastępnik
- 1 liningZastępnik
- 1 setting and daubingZastępnik
Materiały z połączonych planów

10% atrybucji
Mild Steel Plate and Sheet Hammered from a Billet
autor: Forge
Nowoczesny
42
0
0
0
5
0

10% atrybucji
Fireclay Firebricks
autor: Clay
Ceramika i glina
39
0
0
0
4
0

10% atrybucji
Casting Iron in a Cupola Furnace — Re-Melting Pig Iron into Finished Castings
autor: Piett
Obróbka metali
53
0
0
0
6
0

10% atrybucji
Making Coke from Coal — The Smokeless Fuel That Forged the Industrial Revolution
autor: Gimli
Obróbka metali
73
0
0
0
4
0
Według tego planu powstaje
CC0 Domena publiczna
Ten plan jest udostępniany na licencji CC0. Możesz go swobodnie kopiować, modyfikować, rozpowszechniać i wykorzystywać do dowolnych celów, bez konieczności uzyskiwania zgody.
Wesprzyj Makera kupując produkty przez jego plan, za co zarabia Prowizja Makera ustalony przez sprzedawców, lub stwórz nową iterację tego planu i dołącz go jako połączenie w swoim własnym planie, aby dzielić się przychodami.