LDPE Pellets: Ethylene Polymerised at 1500 Atmospheres with a Trace of Oxygen
Polyethylene was discovered at ICI by Fawcett, Gibson and Perrin (US 2,153,553, 1939): ethylene squeezed to over a thousand atmospheres and heated, with a trace of oxygen to start the reaction, turns into a tough, waxy solid that melts at about 120 °C. Their Example III, at 1500 atmospheres and 210 °C for 5 hours, turned 80 % of the ethylene into polymer. The heat of reaction must be carried away, or the gas decomposes explosively. Extruding it into pellets is our step.
The picture: our diagram.
Zaawansowany
About 6 hours
Treści niebezpieczne
Ten blueprint zawiera niebezpieczne procedury. Zaloguj się i włącz niebezpieczne treści w ustawieniach konta, aby zobaczyć instrukcje krok po kroku.
Zaloguj sięWedług tego planu powstaje
Powiązane blueprinty
Te blueprinty dzielą się wiedzą — technikami, materiałami lub zasadami
CC0 Domena publiczna
Ten plan jest udostępniany na licencji CC0. Możesz go swobodnie kopiować, modyfikować, rozpowszechniać i wykorzystywać do dowolnych celów, bez konieczności uzyskiwania zgody.
Wesprzyj Makera kupując produkty przez jego plan, za co zarabia Prowizja Makera ustalony przez sprzedawców, lub stwórz nową iterację tego planu i dołącz go jako połączenie w swoim własnym planie, aby dzielić się przychodami.