Platinum Boat: Cut from Foil and Bent over a Brass Former (Blair, 1888)
Charlie

Autor

Charlie

7. listopad 2026DE
9
0
0
0
0

Platinum Boat: Cut from Foil and Bent over a Brass Former (Blair, 1888)

A small trough of platinum foil that carries a sample into a combustion tube. Andrew Blair (1888): "This boat is made by cutting a piece of platinum-foil in the shape shown in Fig. 65, and bending it up over a brass former into the shape shown in Fig. 64." His pattern is 3.5 long, 1.3 wide at one end and 1.07 at the other, with tabs at each end; the figure does not mark the units. Foil thickness and the former are not given. Source: A. A. Blair, The Chemical Analysis of Iron (1888), p. 129. Picture: Figs. 64-65.
Początkujący
Unknown

Instrukcje

1

Read Blair

"This boat is made by cutting a piece of platinum-foil in the shape shown in Fig. 65, and bending it up over a brass former into the shape shown in Fig. 64."
2

Cut the blank

Cut platinum foil to the pattern of Fig. 65: 3.5 long between the end tabs, 1.3 wide at one end tapering to 1.07 at the other, with a tab .5 wide at the wide end and .37 wide at the narrow end, each flanked by V-notches. The figure does not mark the units, and the foil thickness, and how the foil is made, are not given (unknown).

Materiały do tego kroku:

PlatynaPlatyna1 foil

Potrzebne narzędzia:

Nożyce do blachyNożyce do blachy
Nieznana metoda kształtowaniaNieznana metoda kształtowania
Nieznane wymiaryNieznane wymiary
3

Bend it over the former

Bend the blank up over a brass former into the trough of Fig. 64, folding the end tabs up to close the ends. The shape of the former, and how it is made, are not given (ours: brass round bar as its stock).

Potrzebne narzędzia:

Pręt mosiężny okrągłyPręt mosiężny okrągły
Nieznane wymiaryNieznane wymiary
4

Use

Blair opens out the sides to slide in a moist carbonaceous residue, bends them back into shape, dries the boat and contents at 100 °C, and pushes it into the porcelain or platinum tube to burn off the carbon.

Materiały

1
  • 1 foil
    Zastępnik

Wymagane narzędzia

4

Według tego planu powstaje

CC0 Domena publiczna

Ten plan jest udostępniany na licencji CC0. Możesz go swobodnie kopiować, modyfikować, rozpowszechniać i wykorzystywać do dowolnych celów, bez konieczności uzyskiwania zgody.

Wesprzyj Makera kupując produkty przez jego plan, za co zarabia Prowizja Makera ustalony przez sprzedawców, lub stwórz nową iterację tego planu i dołącz go jako połączenie w swoim własnym planie, aby dzielić się przychodami.

Dyskusja

(0)

Zaloguj się aby dołączyć do dyskusji

Ładowanie komentarzy...