Teaspoon Forged from a Silver Bar (Payne 1914)
Arthur F. Payne · Public domain (1914)
Forge

Autor

Forge

27. październik 2026NO
13
0
0
0
0

Teaspoon Forged from a Silver Bar (Payne 1914)

A 6-inch silver teaspoon forged out of a small bar of silver, the way a blacksmith forges iron. Arthur Payne called it the hardest of his five spoon methods, but the cheapest, because almost no silver is wasted. Source: A. F. Payne, Art Metalwork with Inexpensive Equipment (1914), pp. 184–186; annealing from his chapter XI. Cutting the bar from sheet is ours. Picture: Payne's Fig. 158, teaspoons forged this way.
Zaawansowany
1 day

Instrukcje

1

Cut the silver bar

For a teaspoon 6 in long you need a piece of sterling silver 4 in long, ½ in wide and ⅛ in thick. Mark it out and saw it from sheet of that thickness (cutting from sheet is ours).

Materiały do tego kroku:

Blacha ze srebra sterlingBlacha ze srebra sterling1 piece 4 × ½ × ⅛ in

Potrzebne narzędzia:

Rysik traserskiRysik traserski
Piłka jubilerskaPiłka jubilerska
2

Forge out the bowl

Heat the bar until it is almost red-hot, hold it in tongs and forge the bowl out on the anvil. Silver forges more easily when it is nearly red, but never hammer it while it is red-hot: it will crack.

Potrzebne narzędzia:

Palnik BunsenaPalnik Bunsena
SzczypceSzczypce
KowadłoKowadło
MłotekMłotek
3

Work bowl, then shank and handle

Hammer the bowl until it is hard, then the shank and handle, so the whole spoon is hard before you anneal it again. That saves time.

Potrzebne narzędzia:

KowadłoKowadło
MłotekMłotek
4

Anneal and repeat

To soften it, heat it to a dull red and plunge it into water, or let it cool. Then go on forging until the spoon is roughly to shape.

Materiały do tego kroku:

WodaWoda1 as required

Potrzebne narzędzia:

Palnik BunsenaPalnik Bunsena
SzczypceSzczypce
Naczynie szklaneNaczynie szklane
5

Trim with shears and file

Trim the outline with the shears and file the edges smooth.

Potrzebne narzędzia:

Nożyce do blachy o dużej wytrzymałościNożyce do blachy o dużej wytrzymałości
Pilniki (pilnik ręczny)Pilniki (pilnik ręczny)
6

Polish out the file marks

Rub out all the scratches and file marks with emery cloth.

Potrzebne narzędzia:

Płótno szmerglowePłótno szmerglowe
7

Anneal to even the fire scale

Anneal the spoon thoroughly once more. Heated silver grows a thin white skin, the fire scale, and this brings it back over the spots where filing and polishing took it off, so the colour is even.

Materiały do tego kroku:

WodaWoda1 as required

Potrzebne narzędzia:

Palnik BunsenaPalnik Bunsena
SzczypceSzczypce
Naczynie szklaneNaczynie szklane
8

Planish with smooth hammers

Planish the spoon on smooth tools with smooth, bright hammers. This makes it stiff again after the annealing.

Potrzebne narzędzia:

Młotek do planowaniaMłotek do planowania
KowadłoKowadło
PalikPalik
9

Final polish with rouge

Polish it lightly with a soft cotton flannel and a little red rouge.

Potrzebne narzędzia:

Ściereczka do polerowania biżuteriiŚciereczka do polerowania biżuterii
Czerwień jubilerskaCzerwień jubilerska

Materiały

2

Wymagane narzędzia

14

Według tego planu powstaje

CC0 Domena publiczna

Ten plan jest udostępniany na licencji CC0. Możesz go swobodnie kopiować, modyfikować, rozpowszechniać i wykorzystywać do dowolnych celów, bez konieczności uzyskiwania zgody.

Wesprzyj Makera kupując produkty przez jego plan, za co zarabia Prowizja Makera ustalony przez sprzedawców, lub stwórz nową iterację tego planu i dołącz go jako połączenie w swoim własnym planie, aby dzielić się przychodami.

Dyskusja

(0)

Zaloguj się aby dołączyć do dyskusji

Ładowanie komentarzy...