Smelting Copper from Malachite Ore — Extractive Metallurgy
Forge

Создано

Forge

23. March 2026

Smelting Copper from Malachite Ore — Extractive Metallurgy

Smelt copper from malachite ore (copper carbonate) by heating it with charcoal in a forced-draft furnace. Copper smelting, first practised around 5000 BCE in the Near East, marks the beginning of the metallurgical age. The process uses carbon monoxide from burning charcoal to chemically reduce copper oxide to metallic copper at temperatures above 1085 degrees C.

Advanced
6-10 hours

Инструкции

1

Build the Furnace

Construct a small shaft furnace from clay mixed with sand and chopped straw (the sand and straw improve thermal shock resistance). The furnace is a hollow cylinder approximately 30-40 cm in internal diameter and 50-70 cm tall. Leave an opening at the base for the tuyere — a clay pipe through which the bellows deliver forced air. The tuyere should enter the furnace at a slight upward angle, about 5-10 cm above the base. Leave a tap hole or removable plug at the base on the opposite side from the tuyere for draining slag. Allow the furnace to dry thoroughly before firing — wet clay will crack when heated.

2

Prepare the Ore

Crush the malachite ore to small pieces (roughly 1-2 cm) using a hammerstone on a flat stone anvil. Smaller pieces expose more surface area to the reducing gases, improving the efficiency of the smelt. Malachite (Cu2CO3(OH)2) is a green copper carbonate mineral that is relatively easy to reduce compared to copper sulphide ores — it requires only a carbon monoxide atmosphere at sufficient temperature. Sort out any obvious non-copper rock (gangue) to improve the copper content of your charge. Rich malachite ore contains approximately 57 percent copper by weight.

Step 2 - Image 1
3

Charge and Light the Furnace

Fill the furnace with alternating layers of charcoal and crushed ore — a layer of charcoal 5-8 cm thick, then a layer of ore 2-3 cm thick, repeating until the furnace is full. Light the charcoal from the top and allow it to burn down slowly. Once the charcoal is well alight, begin pumping the bellows to force air through the tuyere. The forced air dramatically increases the combustion temperature. Charcoal burning in a forced-draft furnace reaches 1100-1200 degrees C — well above copper's melting point of 1085 degrees C. The carbon monoxide produced by the charcoal reacts with the copper oxide in the ore, reducing it to metallic copper.

4

Maintain the Smelt

Continue pumping the bellows steadily for 2-4 hours. As the charge descends in the furnace, add more charcoal and ore from the top to maintain the column. The chemical reaction proceeds as: CuO + CO -> Cu + CO2. The released copper collects as small prills (droplets) that sink through the slag to the bottom of the furnace. The slag — a glassy mixture of iron oxide, silica, and other impurities — floats on top of the denser copper. If the furnace has a tap hole, periodically drain the molten slag to prevent it from clogging the furnace. The smelt is complete when all the ore has been consumed.

Step 4 - Image 1
5

Extract and Refine the Copper

Allow the furnace to cool, then break it open to extract the copper. The copper typically forms a rough, spongy mass (called a bun or plano-convex ingot) at the base, with slag adhering to the top and sides. Separate the copper from the slag by hammering — slag is brittle and shatters, while copper is malleable and deforms. For purer copper, re-melt the crude bun in a clay crucible with fresh charcoal and skim the slag off the surface. The resulting copper is typically 95-98 percent pure and can be hammered, cast, or alloyed with tin to make bronze. A successful smelt from rich malachite yields approximately 200-400 g of copper per kilogram of ore.

Материалы

  • Malachite ore (copper carbonate, Cu2CO3(OH)2) - 2-5 kg of crushed ore pieceЗаполнитель
    Просмотр
  • Hardwood charcoal - 10-20 kg pieceЗаполнитель
    Просмотр
  • Clay (for furnace construction) - 20-30 kg pieceЗаполнитель
    Просмотр
  • Sand (mixed with clay for refractory lining) - 5 kg pieceЗаполнитель
    Просмотр

Требуемые инструменты

  • Bellows (leather bag with clay tuyere)Заполнитель
    Просмотр
  • Hammerstone (for crushing ore)Заполнитель
    Просмотр
  • Stone tongs or green wood tongs

CC0 Общественное достояние

Этот чертёж выпущен под лицензией CC0. Вы можете свободно копировать, изменять, распространять и использовать эту работу в любых целях без запроса разрешения.

Поддержите мейкера, покупая товары через его чертёж, где он получает Комиссию мейкера установленную продавцами, или создайте новую итерацию этого чертежа и включите его как связь в свой чертёж для распределения дохода.

Обсуждение

(0)

Войти чтобы присоединиться к обсуждению

Загрузка комментариев...