Blown Glass Jar with a Cork Lid
Forge

Создано

Forge

11. октябрь 2026NO
41
0
0
0
0

Blown Glass Jar with a Cork Lid

A jar is blown like a bottle, but instead of a narrow neck its mouth is opened out on the pontil to nearly the full width of the body, with straight walls and a flat base so it stands and can be filled with a spoon. A wide cork punched from bark makes the lid. All furnace work, the gather, the pontil and the annealing follow the bottle blueprint.
Продвинутый
Half a day, plus annealing

Инструкции

1

Gather, blow, pontil and anneal

The furnace, gathering, transfer to the pontil and annealing, step by step.
2

Blow a straight-sided bubble

Gather soda-lime glass, marver it into a cylinder and blow a bubble. Roll it on the marver to keep the walls straight and press the end flat on the marver for the base.

Материалы для этого шага:

Натриево-кальциевое стеклоНатриево-кальциевое стекло1 кг

Необходимые инструменты:

Стекловаренная печь, способная нагреваться до 1100 градусов ЦельсияСтекловаренная печь, способная нагреваться до 1100 градусов Цельсия
Стеклодувная трубкаСтеклодувная трубка
Марвер (плита для выкатки стекла)Марвер (плита для выкатки стекла)
Скамья стеклодуваСкамья стеклодува
Термостойкие перчаткиТермостойкие перчатки
Защитные очкиЗащитные очки
3

Mark the shoulder

Score a line with the jacks where the mouth will be, just beyond the full width of the body.

Необходимые инструменты:

Щипцы стеклодуваЩипцы стеклодува
Скамья стеклодуваСкамья стеклодува
4

Transfer to the pontil

Attach the pontil to the base, crack the jar off the blowpipe at the scored line.

Необходимые инструменты:

ПонтияПонтия
Скамья стеклодуваСкамья стеклодува
5

Open the mouth

Reheat the open end and, turning the pontil on the bench rails, open it with the jacks until the mouth is as wide as the body. Fire-polish the rim smooth in the furnace.

Необходимые инструменты:

Щипцы стеклодуваЩипцы стеклодува
Стекловаренная печь, способная нагреваться до 1100 градусов ЦельсияСтекловаренная печь, способная нагреваться до 1100 градусов Цельсия
Скамья стеклодуваСкамья стеклодува
6

Crack off and anneal

Crack the jar off the pontil straight into the annealing oven and anneal it as for the bottle.

Необходимые инструменты:

Печь для отжигаПечь для отжига
Термостойкие перчаткиТермостойкие перчатки
7

Grind the pontil mark

When cold, grind the pontil scar on the base smooth on wet abrasive so it stands flat.

Необходимые инструменты:

Лист наждачной бумагиЛист наждачной бумаги
Точильный каменьТочильный камень
8

Cut a cork lid

Measure the mouth's inside diameter. Punch a cork a little wider than it from thick, boiled cork bark with the cork borer, and taper its lower edge so it presses in.

Материалы для этого шага:

Пласт пробковой корыПласт пробковой коры0.1 кг

Необходимые инструменты:

Цифровой штангенциркуль 6 дюймовЦифровой штангенциркуль 6 дюймов
ПробкосверлоПробкосверло
Строительный ножСтроительный нож
Лист наждачной бумагиЛист наждачной бумаги
9

Troubleshooting

Jar blowing troubleshooting.

Flow

Loading...

Материалы

2

Требуемые инструменты

14

CC0 Общественное достояние

Этот чертёж выпущен под лицензией CC0. Вы можете свободно копировать, изменять, распространять и использовать эту работу в любых целях без запроса разрешения.