Strontium Ferrite Disc Magnet: 0.8 mol SrCO3 to 3.2 mol Iron Oxide, 1280 °C (Went, Philips 1956, Ex. 11)

Strontium Ferrite Disc Magnet: 0.8 mol SrCO3 to 3.2 mol Iron Oxide, 1280 °C (Went, Philips 1956, Ex. 11)

от CharlieDE

Материалы

9
0
0
0
0
0
Strontium Ferrite Disc Magnet: 1 mol SrCO3 to 3 mol Iron Oxide, 1220 °C (Went, Philips 1956, Ex. 10)

Strontium Ferrite Disc Magnet: 1 mol SrCO3 to 3 mol Iron Oxide, 1220 °C (Went, Philips 1956, Ex. 10)

от CharlieDE

Материалы

9
0
0
0
0
0
Strontium Ferrite Disc Magnet: 1 mol SrCO3 to 2.5 mol Iron Oxide, 1200 °C (Went, Philips 1956, Ex. 9)

Strontium Ferrite Disc Magnet: 1 mol SrCO3 to 2.5 mol Iron Oxide, 1200 °C (Went, Philips 1956, Ex. 9)

от CharlieDE

Материалы

5
0
0
0
0
0
Strontium Ferrite Disc Magnet: Presintered at 1100 °C, 0.1 mol SrCO3 to 0.7 mol Iron Oxide (Went, Philips 1956, Ex. 8)

Strontium Ferrite Disc Magnet: Presintered at 1100 °C, 0.1 mol SrCO3 to 0.7 mol Iron Oxide (Went, Philips 1956, Ex. 8)

от CharlieDE

Материалы

8
0
0
0
0
0
Strontium Ferrite Disc Magnet: Presintered at 1100 °C, 0.2 mol SrCO3 to 1.1 mol Iron Oxide (Went, Philips 1956, Ex. 7)

Strontium Ferrite Disc Magnet: Presintered at 1100 °C, 0.2 mol SrCO3 to 1.1 mol Iron Oxide (Went, Philips 1956, Ex. 7)

от CharlieDE

Материалы

8
0
0
0
0
0
Barium Ferrite Disc Magnet: 0.4 mol BaCO3 to 3.7 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 6)

Barium Ferrite Disc Magnet: 0.4 mol BaCO3 to 3.7 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 6)

от CharlieDE

Материалы

8
0
0
0
0
0
Barium Ferrite Disc Magnet: 0.4 mol BaCO3 to 3.2 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 5)

Barium Ferrite Disc Magnet: 0.4 mol BaCO3 to 3.2 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 5)

от CharlieDE

Материалы

6
0
0
0
0
0
Barium Ferrite Disc Magnet: 0.5 mol BaCO3 to 3.5 mol Iron Oxide, 10 Minutes at 1330 °C (Went, Philips 1956, Ex. 4)

Barium Ferrite Disc Magnet: 0.5 mol BaCO3 to 3.5 mol Iron Oxide, 10 Minutes at 1330 °C (Went, Philips 1956, Ex. 4)

от CharlieDE

Материалы

6
0
0
0
0
0
Barium Ferrite Disc Magnet: 1 mol BaCO3 to 3.5 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 3)

Barium Ferrite Disc Magnet: 1 mol BaCO3 to 3.5 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 3)

от CharlieDE

Материалы

7
0
0
0
0
0
Barium Ferrite Disc Magnet: 1 mol BaCO3 to 3 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 2)

Barium Ferrite Disc Magnet: 1 mol BaCO3 to 3 mol Iron Oxide, 1330 °C (Went, Philips 1956, Ex. 2)

от CharlieDE

Материалы

7
0
0
0
0
0
Barium Ferrite Disc Magnet: 1 mol BaCO3 to 2.5 mol Iron Oxide, 1310 °C (Went, Philips 1956, Ex. 1)

Barium Ferrite Disc Magnet: 1 mol BaCO3 to 2.5 mol Iron Oxide, 1310 °C (Went, Philips 1956, Ex. 1)

от CharlieDE

Материалы

5
0
0
0
0
0
Ferrite Toroid Core: Nickel-Zinc Ferrite, Then 3 Days at 950 °C in Oxygen (Snoek 1948, Ex. III)
Опасно

Ferrite Toroid Core: Nickel-Zinc Ferrite, Then 3 Days at 950 °C in Oxygen (Snoek 1948, Ex. III)

от CharlieDE

Материалы

4
0
0
0
0
0
Ferrite Toroid Core: Magnesium-Zinc Ferrite, One-Day Grind, 1400 °C (Snoek 1948, Ex. II)

Ferrite Toroid Core: Magnesium-Zinc Ferrite, One-Day Grind, 1400 °C (Snoek 1948, Ex. II)

от CharlieDE

Материалы

7
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

5
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

8
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

5
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

2
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

2
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

9
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

3
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

3
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

6
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

6
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

от CharlieDE

Материалы

7
0
0
0
0
0
Показано 24 из 460