Indium: From Freiberg Zinc, Thrown Down on Undissolved Zinc, Purified as Sulphite and Reduced in Hydrogen (Roscoe 1913)
Freiberg zinc carries a trace of indium. Dissolve most of the zinc in acid and the indium plates out on the zinc that is left. Acids and ammonia then strip away the other metals, sodium bisulfite throws the indium down as a sulphite, heat turns it to oxide, and hydrogen takes the oxygen away.
Result: white, soft indium metal, softer than lead, melting at 155 °C.
Source: Roscoe and Schorlemmer, A Treatise on Chemistry vol. 2 (1913), p. 754. Unknown: the indium-bearing zinc; no blueprint smelts it yet. Not given: amounts. Sulphur dioxide is a poison gas. Picture drawn by Youblob.
Hejuru
5 days
Ibirimo biteje akaga
Iki gikorwa kirimo imikorere yangiza. Injira hanyuma ufungure ibikoresho byangiza mu igenamiterere ryawe kugira ngo urebe amabwiriza.
InjiraIki gishushanyo gikora
CC0 Umurenge rusange
Iyi blueprint yasohowe munsi ya CC0. Ushobora gukoporora, guhindura, gukwirakwiza no gukoresha nta kwemererwa.
Shyigikira Umuremyi ugura ibicuruzwa binyuze muri Blueprint ye Komisiyo y'Umuremyi byashyizweho n'Abacuruzi, cyangwa kora verisiyo nshya y'iyi Blueprint ukayinjiza nk'isano muri Blueprint yawe kugira ngo musangire inyungu.