Continuous Casting of Steel Billets
In continuous casting, molten steel is poured without stop into a short, open-bottomed copper mould and drawn out below as a solid strand. The steel goes from the ladle to a tundish, which holds a reserve while ladles are changed and steadies the flow, and from there into the water-cooled mould. The mould oscillates so the steel does not stick, and a lubricating powder melts on the surface and traps slag. A thin skin freezes against the copper; the strand leaves the mould still liquid inside, is held by water-cooled rolls and sprayed with water until it is solid, then straightened and cut to length. Billet casters cast sections under 200 mm square, up to 12 m long, at up to 4 m a minute.
متقدم
Factory process
التعليمات
1
1
Ladle to tundish
Ladle to tundish
Bring the ladle of molten steel to the casting machine and pour through a refractory shroud into the tundish, which buffers the metal while ladles are changed and smooths the flow.
المواد لهذه الخطوة:
فولاذ مصهور1 as requiredالأدوات المطلوبة:
مِغرفة صبّ المعدن
الحوض الوسيط (تنديش)2
2
Mould
Mould
Let the steel run from the tundish through a submerged entry nozzle into the open-base copper mould, 0.5–2 m deep, cooled by water and oscillating vertically. Add the lubricant powder, which melts, stops sticking and floats slag to the top.
المواد لهذه الخطوة:
مسحوق القالب1 as requiredالأدوات المطلوبة:
قالب صبّ نحاسي مبرَّد بالماء3
3
Spray chamber
Spray chamber
The strand leaves the mould with a solid shell and a liquid core. Support it on closely spaced water-cooled rolls and spray it with water until it solidifies.
الأدوات المطلوبة:
حجرة رشّ ذات أسطوانات دعم4
4
Straighten, withdraw and cut
Straighten, withdraw and cut
Pass the strand through the straightening and withdrawal rolls, then cut it into billets of set length with shears or a travelling oxyacetylene torch, and mark them.
الأدوات المطلوبة:
أسطوانات التقويم والسحب
موقد قطع أوكسي أسيتيلينالمواد
2- 1 as requiredعنصر نائب
- 1 as requiredعنصر نائب
الأدوات المطلوبة
6- عنصر نائب
- عنصر نائب
- عنصر نائب
- عنصر نائب
- عنصر نائب
- عنصر نائب
هذا المخطط يصنع
المخططات ذات الصلة
هذه المخططات تشارك المعرفة مع هذا — التقنيات والمواد والمبادئ
CC0 ملكية عامة
هذا المخطط مُصدر بموجب CC0. يحق لك نسخه وتعديله وتوزيعه واستخدامه لأي غرض، دون طلب إذن.
ادعم الصانع بشراء منتجات عبر مخططه حيث يكسب عمولة الصانع يحددها البائعون، أو أنشئ نسخة جديدة من هذا المخطط وضمّنه كرابط في مخططك لمشاركة الإيرادات.