Semi-Cured Phenolic Sheet: Paper Dipped in Phenol Resin and Part-Cured at 120-130 °C (Lucas, Western Electric, US 1,470,990)

Paper soaked in phenol resin is dried, then cured only part of the way, so the resin is stiff but not yet hard. Lucas did this before the final hot press so the press would not squeeze the resin out of the fibres. Result: a dry, partly cured phenolic sheet that a later coat of phenolic resin can still bond into. Source: Lucas, US 1,470,990 (Western Electric, 1923). Stopping before his final hot press is ours. Not given: the solvent in his resin, paper grade, mercerising strengths. Picture drawn by Youblob.
متوسط
1 hour

التعليمات

1

Dip the paper in phenol resin

Run the paper through a bath of phenol resin of specific gravity about 0.970: about 2 minutes for plain paper, 1 minute or less if mercerised first. Ours: Liquid Bakelite as the resin; Lucas does not say how it was thinned.

المواد لهذه الخطوة:

ورقورق1 as required
باكليت سائل (ناتج تكاثف الفينول والفورمالديهيد)باكليت سائل (ناتج تكاثف الفينول والفورمالديهيد)1 as required

الأدوات المطلوبة:

خط تشريب البريبريغخط تشريب البريبريغ
مقياس كثافةمقياس كثافة
2

Optional: mercerise the paper first

For faster, fuller soaking, first pass the paper through caustic soda, squeeze, wash in water, neutralise in an acid, wash again and dry. Strengths and the acid: not given.

الأدوات المطلوبة:

الصودا الكاوية (هيدروكسيد الصوديوم)الصودا الكاوية (هيدروكسيد الصوديوم)
خط تشريب البريبريغخط تشريب البريبريغ
3

Dry at about 90 °C

Dry the soaked paper in an oven at about 90 °C, just long enough to dry it.

الأدوات المطلوبة:

فرن تجفيففرن تجفيف
4

Part-cure at 120-130 °C

Pass the dry paper through a curing oven at 120-130 °C for about 10 minutes (Lucas's description; his claim 4 says 125 °C for about 10 seconds). The resin sets as stiff as the fibres, but does not harden through.

الأدوات المطلوبة:

فرن معالجةفرن معالجة
5

Dip again for 10-15 seconds and dry

Dip the part-cured paper in phenol resin again for 10-15 seconds, then dry at about 90 °C until it can be wound on a reel. Stop here: the sheet is semi-cured. Lucas's next step, stacking and hot pressing, cures it fully.

المواد لهذه الخطوة:

باكليت سائل (ناتج تكاثف الفينول والفورمالديهيد)باكليت سائل (ناتج تكاثف الفينول والفورمالديهيد)1 as required

الأدوات المطلوبة:

خط تشريب البريبريغخط تشريب البريبريغ
فرن تجفيففرن تجفيف

المواد

2

الأدوات المطلوبة

5

المخططات ذات الصلة

هذه المخططات تشارك المعرفة مع هذا — التقنيات والمواد والمبادئ

CC0 ملكية عامة

هذا المخطط مُصدر بموجب CC0. يحق لك نسخه وتعديله وتوزيعه واستخدامه لأي غرض، دون طلب إذن.

ادعم الصانع بشراء منتجات عبر مخططه حيث يكسب عمولة الصانع يحددها البائعون، أو أنشئ نسخة جديدة من هذا المخطط وضمّنه كرابط في مخططك لمشاركة الإيرادات.

النقاش

(0)

تسجيل الدخول للمشاركة في النقاش

جارٍ تحميل التعليقات...