Edward E. Simmons, Jr. of Pasadena patented the bonded wire strain gauge in 1942, US 2,292,549 (filed 1940). A very fine resistance wire is cemented to a member along its entire length, so it stretches and shortens exactly with the surface and its electrical resistance follows the strain. His preferred form: Constantan or Advance wire, about 0.003 inch, wound back and forth on a thin paper, set in Glyptal, then cemented to the member and calibrated.
İleri
Workshop process
Talimatlar
1
1
Wind the filament on thin paper
Wind the filament on thin paper
Use a fine resistance wire such as Constantan or Advance (a copper-nickel alloy, about 45 % nickel and 55 % copper); Simmons used No. 40 gauge, about 0.0031 inch. Wind it back and forth across a thin paper in parallel lengths whose alternate ends are joined, the strands very close together but not touching. A winding jig keeps the filament slightly taut.
Bu adım için malzemeler:
Konstantan tel1 as required
Kağıt1 yaprakGerekli aletler:
Sarma aparatı
Makas2
2
Set it in Glyptal
Set it in Glyptal
Cover the wound filament with Glyptal and let it dry and harden thoroughly. Filament and paper now form one gauge unit, the filament lying in the plane of the paper surface.
Bu adım için malzemeler:
Glyptal alkid reçinesi1 as requiredGerekli aletler:
İnce fırçalar
Kurutma fırını3
3
Cement it to the member
Cement it to the member
Put Glyptal on the surface of the member and wrap the gauge unit on with the strands running in the direction of the strain to be measured, the paper outside. The small amount of Glyptal on the surface insulates the filament from the member. Hold filament and paper in place by wrapping them with thread, then dry and harden the Glyptal thoroughly.
Bu adım için malzemeler:
Glyptal alkid reçinesi1 as required
Pamuk İplik1 as requiredGerekli aletler:
İnce fırçalar
Kurutma fırını
Makas4
4
Calibrate it
Calibrate it
Load the member progressively in a materials testing machine and note the change in the filament's resistance at each load, measured on a Wheatstone bridge in which the filament is one arm. For very fast loads, as in impact tests, an oscillograph takes the place of the galvanometer.
Gerekli aletler:
Malzeme test makinesi
Wheatstone köprüsü
Analog galvanometre5
5
Bonding area and signal size
Bonding area and signal size
Jupyter defteri yükleniyor…
Malzemeler
4- 1 as requiredYer Tutucu
- 1 yaprakYer Tutucu
- 1 as requiredYer Tutucu
- 1 as requiredYer Tutucu
Gerekli Aletler
7- Yer Tutucu
- Yer Tutucu
- Yer Tutucu
- Yer Tutucu
- Yer Tutucu
- Yer Tutucu
- Yer Tutucu
Bu planla yapılan
İlgili Blueprint'ler
Bu blueprint'ler bilgi paylaşır — teknikler, malzemeler veya ilkeler
CC0 Kamu Malı
Bu plan CC0 lisansıyla yayınlanmıştır. İzin almadan kopyalayabilir, değiştirebilir, dağıtabilir ve herhangi bir amaçla kullanabilirsiniz.
Planı üzerinden ürün satın alarak Maker'ı destekleyin, böylece Maker Komisyonu Satıcılar tarafından belirlenen komisyonu kazanırlar veya bu Planın yeni bir versiyonunu oluşturun ve gelir paylaşımı için kendi Planınıza bağlantı olarak ekleyin.