Nichrome Wire: Nickel and Chromium Fused, Drawn and Annealed
Forge

Oluşturan

Forge

18. Ekim 2026NO
13
0
0
0
0

Nichrome Wire: Nickel and Chromium Fused, Drawn and Annealed

Nichrome is the heating wire of toasters and irons. Albert Marsh patented it in 1906: nickel with less than 25 % chromium, drawn into wire and annealed, with about fifty times the resistance of copper and great resistance to oxidation when hot. Iron, he wrote, will not do. Elwood Haynes (1907) fused pure, carbon-free nickel and chromium in a magnesia crucible under an oxyhydrogen flame. White heat: face shield and gloves. The picture: Marsh's patent drawing, a rheostat wound with the alloy (US 811,859).
İleri
3 days

Talimatlar

1

Weigh 85 nickel to 15 chromium

Cut 85 g of nickel sheet into small pieces and weigh 15 g of chromium: Marsh's own example. Both must be pure and free of carbon.

Bu adım için malzemeler:

Nikel levhaNikel levha85 g
Krom MetaliKrom Metali15 g

Gerekli aletler:

Metal makasıMetal makası
Eşit kollu teraziEşit kollu terazi
2

Fuse under the oxyhydrogen flame

Put the metals in a magnesia crucible, set it in a furnace lined with magnesia, and heat it with the oxyhydrogen blowpipe until both have melted together.

Gerekli aletler:

Magnezya PotaMagnezya Pota
Magnezyum oksitMagnezyum oksit
Oksihidrojen ÜfleciOksihidrojen Üfleci
Pota MaşasıPota Maşası
Yüz SiperliğiYüz Siperliği
Deri EldivenDeri Eldiven
3

Cast a rod

Pour the alloy into a narrow mould to get a rod that will start in the largest hole of the drawplate.

Gerekli aletler:

Külçe kalıbıKülçe kalıbı
Pota MaşasıPota Maşası
Yüz SiperliğiYüz Siperliği
Deri EldivenDeri Eldiven
4

Draw and anneal

Draw the rod down through the drawplate one hole at a time, as in the drawplate blueprint, and anneal it in the furnace whenever it gets hard. Marsh gives no annealing temperature. Stop at 0.41 mm (0.016 in).

Gerekli aletler:

Çelik haddeleme plakasıÇelik haddeleme plakası
Çekme kerpeteniÇekme kerpeteni
Tel çekme yağlayıcısıTel çekme yağlayıcısı
Odun Kömürü FırınıOdun Kömürü Fırını
MikrometreMikrometre
Deri EldivenDeri Eldiven
5

Check the resistance

Measure one metre with the multimeter. Marsh's 15 % wire of this size measured about 2.3 ohms per foot, which is 7.5 ohms per metre.

Gerekli aletler:

MultimetreMultimetre

Malzemeler

2

Gerekli Aletler

15

İlgili Blueprint'ler

Bu blueprint'ler bilgi paylaşır — teknikler, malzemeler veya ilkeler

CC0 Kamu Malı

Bu plan CC0 lisansıyla yayınlanmıştır. İzin almadan kopyalayabilir, değiştirebilir, dağıtabilir ve herhangi bir amaçla kullanabilirsiniz.

Planı üzerinden ürün satın alarak Maker'ı destekleyin, böylece Maker Komisyonu Satıcılar tarafından belirlenen komisyonu kazanırlar veya bu Planın yeni bir versiyonunu oluşturun ve gelir paylaşımı için kendi Planınıza bağlantı olarak ekleyin.

Tartışma

(0)

Giriş yapın tartışmaya katılmak için

Yorumlar yükleniyor...