Platinum Reforming Catalyst: 0.1 % Platinum and 1.5 % Fluorine on Alumina (Haensel, UOP, US 2,479,110)
Haensel's reforming catalyst: a trace of platinum, only 0.1 %, on alumina that also carries fluorine. The fluorine is what makes it work: on the same naphtha it lifted the reformate from octane 59.8 to 78.8.
Variable: fluorine content. Tested on a Pennsylvania naphtha of octane 41.8: no fluorine 59.8; 1.5 % 78.8 (874 °F); 3 % 77.4 (824 °F); 6 % 72.4 (755 °F). Keep it at about 3 % or below.
Source: Haensel, US 2,479,110 (1949), Ex. I-II and IV. Not given: amounts of the aluminium salt and ammonia. Unknown: how the aluminium chloride hexahydrate, chloroplatinic acid and hydrogen sulfide are made. Danger: hydrofluoric acid and hydrogen sulfide are deadly poisons. Picture drawn by Youblob.
Експерт
3 days
Небезпечний контент
Це креслення містить небезпечні процедури. Увійдіть та увімкніть небезпечний контент у налаштуваннях облікового запису, щоб переглянути покрокові інструкції.
УвійтиЗа цим кресленням виготовляють
Пов'язані креслення
Ці креслення діляться знаннями — техніки, матеріали або принципи
CC0 Суспільне надбання
Це креслення випущено під ліцензією CC0. Ви можете вільно копіювати, змінювати, поширювати та використовувати цю роботу для будь-яких цілей без запиту дозволу.
Підтримайте мейкера, купуючи продукти через його креслення, де він отримує Комісію мейкера встановлену вендорами, або створіть нову ітерацію цього креслення та включіть його як зв'язок у власне креслення для розподілу доходу.