Smith's Fire Rake (Poker): a 3/8 in. Rod Drawn to a Flat Point, Crooked, and Looped Over the Anvil (Edwinson, 1886)
Forge

Created by

Forge

14. November 2026NO
8
0
0
0
0

Smith's Fire Rake (Poker): a 3/8 in. Rod Drawn to a Flat Point, Crooked, and Looped Over the Anvil (Edwinson, 1886)

The first job George Edwinson set his readers in Amateur Work (1886): the smith's rake for the forge fire, which "might be dubbed a poker". A yard of 3/8 in. iron rod drawn to a square then flat point with quarter turns, bent into a crook, and the other end bent round in three heats into a loop handle.
Beginner
An hour at the forge

Instructions

1

His sizes

Loading Jupyter Notebook...
2

Read Edwinson

"The rake, Fig. 16, might be dubbed a poker, and as this is the most simple tool, we will deal with that first."
3

Light a small fire

Pile slack round the tuyere, scoop a shallow pit in front of it, put in shavings with a few cinders on top, light and blow gently. Draw slack in until the heap glows, then damp the outside so the fire stays within 6 in. (15 cm) of the tuyere.

Materials for this step:

Bituminous CoalBituminous Coal1 piece

Tools needed:

Blacksmith ForgeBlacksmith Forge
4

Draw the point

Cut 36 in. (91 cm) of 3/8 in. (10 mm) iron rod with a cold chisel. Heat 2 in. of one end glowing white. On the outer edge of the anvil, hammer it lightly on the tip, giving the rod a quarter turn after each blow and drawing it back, to a square point. Strike only while it glows; reheat at a dull red. Next heat, round the corners and draw a flat tapering point (fig. 17).

Materials for this step:

Wrought Iron BarWrought Iron Bar1 piece

Tools needed:

Cold ChiselCold Chisel
Blacksmith ForgeBlacksmith Forge
AnvilAnvil
HammerHammer
5

Crook the end

Heat the point to a dull red and bend it over the outer edge of the anvil with a few light blows into the crook (fig. 16).

Tools needed:

Blacksmith ForgeBlacksmith Forge
AnvilAnvil
HammerHammer
6

Bend the loop

Heat the rod about 10 in. from the other end to redness and bend it over the anvil edge (fig. 18). Heat 3 in. more of the bent part and shape it (fig. 19). Heat again and bring the end round to touch the shoulder (fig. 20), then shape the loop hot with light blows. (Experienced smiths scarf the end and weld it to the shoulder.)

Tools needed:

Blacksmith ForgeBlacksmith Forge
AnvilAnvil
HammerHammer
7

Troubleshooting

Rake troubleshooting.

Flow

Loading...
8

History and honest limits

From George Edwinson, "Smithing and Forging" II, **Amateur Work, Illustrated**, vol. V (1886), pp. 211-213 and figs. 15-20 (checked on the archive.org scan amateurworkillus05lond). Metric figures and the tools are ours.

Materials

2

Tools Required

4

Related Blueprints

These blueprints share knowledge with this one — techniques, materials, or principles that connect them in the learning graph.

CC0 Public Domain

This blueprint is released under CC0. You are free to copy, modify, distribute, and use this work for any purpose, without asking permission.

Support the Maker by purchasing products through their Blueprint where they earn a Maker Commission set by Vendors, or create a new iteration of this Blueprint and include it as a connection in your own Blueprint to share revenue.

Discussion

(0)

Log in to join the discussion

Loading comments...