Nickel-Metal-Hydride Electrode
Jungner's cell, eighty-seven years later, with the cadmium taken out.
The positive electrode is unchanged - nickel oxyhydroxide, exactly as it was in 1899, exactly as it is in the NiCd blueprint earlier in this chain. The electrolyte is the same potassium hydroxide, still taking no part. What changed is the negative, and the change is a genuinely strange idea: instead of a metal that oxidises, use a metal that **absorbs hydrogen** and give it the hydrogen back on demand.
On discharge, MH + OH- gives M + H2O + e-. On charge it runs backwards. The hydrogen lives inside the metal lattice between charge and discharge, and the metal itself is not consumed - which is the same idea as the lithium cobalt oxide in the previous blueprint, arrived at from a completely different direction. Overall: Ni(OH)2 + MH gives NiOOH + M + H2O, and once again the hydroxide and the water cancel out.
**US 4,623,597**, Krishna Sapru, Benjamin Reichman, Arie Reger and Stanford R. Ovshinsky, assigned to Energy Conversion Devices, priority 28. April 1982, filed 25. November 1985, granted 18. November 1986. It claims "a hydrogen rechargeable anode of a disordered non-equilibrium multicomponent material".
**That word "disordered" is the invention.** Conventional materials science says make the crystal as perfect as you can. Ovshinsky spent a career arguing the opposite: a perfect crystal offers every hydrogen atom an identical site, so it works beautifully at one temperature and one pressure and poorly everywhere else. Spoil the order deliberately - many elements, no long-range structure - and you get a SPREAD of binding sites. Slightly worse at the optimum, far better across the range of conditions a real battery actually meets.
The result gives two to three times the capacity of a NiCd cell of the same size, contains no cadmium, and is what was in almost every rechargeable AA sold between the mid-1990s and the arrival of cheap lithium.
**What you build here.** A working cell, with the hydride electrode HARVESTED from a spent commercial cell rather than synthesised - AB5 alloys need arc melting under argon, and recovering a working electrode from something on its way to a recycling bin is both achievable and the more interesting exercise. The positive electrode you make yourself, by the same route as the Jungner blueprint.
Nickel compounds are toxic as dust and the electrolyte is severely caustic. Gated for the first.
Intermediate
4 hours, plus a week of self-discharge measurement
Hazardous content
This blueprint contains hazardous procedures. Log in and enable hazardous content in your account settings to view the step-by-step instructions.
Related Blueprints
These blueprints share knowledge with this one — techniques, materials, or principles that connect them in the learning graph.
CC0 Public Domain
This blueprint is released under CC0. You are free to copy, modify, distribute, and use this work for any purpose, without asking permission.
Support the Maker by purchasing products through their Blueprint where they earn a Maker Commission set by Vendors, or create a new iteration of this Blueprint and include it as a connection in your own Blueprint to share revenue.