Zirconium: Oxide Reduced with Calcium and Calcium Chloride in a Sealed Bomb at 950 °C (Kiernan, US 1,760,413)
Pure zirconium nitrate is burnt to oxide, then sealed in a steel bomb with clean calcium chips and calcium chloride and held at 950 °C. Water washes out the calcium chloride and dilute nitric acid the lime, leaving zirconium powder.
Result: dark grey zirconium metal powder, passing 150 mesh.
Source: J. W. Kiernan (Westinghouse), US patent 1,760,413, pp. 2-3. Picture drawn by Youblob.
Advanced
3 days
Hazardous content
This blueprint contains hazardous procedures. Log in and enable hazardous content in your account settings to view the step-by-step instructions.
Sign inThis blueprint makes
Related Blueprints
These blueprints share knowledge with this one — techniques, materials, or principles that connect them in the learning graph.
CC0 Public Domain
This blueprint is released under CC0. You are free to copy, modify, distribute, and use this work for any purpose, without asking permission.
Support the Maker by purchasing products through their Blueprint where they earn a Maker Commission set by Vendors, or create a new iteration of this Blueprint and include it as a connection in your own Blueprint to share revenue.