Dysprosium: Oxide Reduced with Lanthanum Turnings at 1650 °C in High Vacuum, Metal Distilled Off (Sanden, Ames 1973)
Nguy hiểm
Charlie

Tạo bởi

Charlie

1. tháng Mười Một 2026DE
1
0
0
0
0

Dysprosium: Oxide Reduced with Lanthanum Turnings at 1650 °C in High Vacuum, Metal Distilled Off (Sanden, Ames 1973)

Lanthanum holds oxygen more tightly than dysprosium does and is much less volatile. Heated together in a tantalum boiler under high vacuum, lanthanum takes the oxygen and dysprosium vapour rises through baffles onto a condenser, leaving lanthanum oxide behind. Result: 125-155 g of dysprosium per run, 56-81 % yield. Source: B. L. Sanden, A study of the reduction of dysprosium oxide with lanthanum (Iowa State University / Ames Laboratory, 1973), pp. 12-27. Work at 1650 °C in high vacuum; hot hydrochloric acid for cleaning. Picture drawn by Youblob.
Nâng cao
1 week

Nội dung nguy hiểm

Blueprint này chứa các quy trình nguy hiểm. Đăng nhập và bật nội dung nguy hiểm trong cài đặt tài khoản của bạn để xem hướng dẫn từng bước.

Đăng nhập

Bản thiết kế này làm ra

Blueprint liên quan

Các blueprint này chia sẻ kiến thức — kỹ thuật, vật liệu hoặc nguyên tắc

CC0 Phạm vi công cộng

Bản thiết kế này được phát hành theo CC0. Bạn tự do sao chép, sửa đổi, phân phối và sử dụng cho bất kỳ mục đích nào mà không cần xin phép.

Hỗ trợ nhà sáng tạo bằng cách mua sản phẩm qua bản thiết kế, nơi họ nhận Hoa hồng nhà sáng tạo do nhà bán hàng đặt, hoặc tạo phiên bản mới và kết nối trong bản thiết kế riêng để chia sẻ doanh thu.

Thảo luận

(0)

Đăng nhập để tham gia thảo luận

Đang tải bình luận...