Plastic Extruder: Steam-Jacketed Screw Stuffer with a Heated Nozzle (Andersen & Strasdin, US 2,384,521, 1945)
A screw extruder for thermoplastics: a turning screw in a steam-jacketed barrel pushes hot, softened plastic forward through a short nozzle heated electrically. The barrel is kept a little below the plastic's flow temperature and the nozzle well above it, so the extruded rod comes out with a smooth, glass-like skin.
Result: an extruder that makes rod, tube or strip at 25 to 30 feet a minute.
Source: B. Andersen and R. F. Strasdin (Celanese), US 2,384,521 (1945). Unknown: sizes and metals. Picture: the patent drawing.
Nâng cao
Unknown
Hướng dẫn
1
1
Make the screw
Make the screw
Turn a screw to fit the barrel. Its thread may be single or double; to press the plastic harder toward the nozzle, make the pitch increase or the groove get shallower toward that end. Example: a double-thread screw. Ours: mild steel. Not given: sizes.
Vật liệu cho bước này:
Thanh tròn thép mềm1 screwCông cụ cần thiết:
Máy tiện kim loại
Máy phay
Kích thước chưa rõ2
2
Make the jacketed barrel
Make the jacketed barrel
Make the barrel with a steam jacket round it and a steam port into the jacket, and a feed throat at the back end. The inside wall may be grooved, pitched so that every flight of the screw always meets a groove; this stops the plastic slipping. Not given: the metal, the steam pressure.
Vật liệu cho bước này:
Kim loại chưa rõ1 barrel and jacketCông cụ cần thiết:
Máy tiện kim loại
Kích thước chưa rõ3
3
Fit the heated nozzle
Fit the heated nozzle
At the front, fit a streamlined nozzle head so no plastic can pocket and decompose, and a nozzle 1/2 to 18 inches long; about 6 inches in the example. Perforated plates may go between the screw and the nozzle. Heat the nozzle with an electric resistance coil. Ours: nichrome wire.
Vật liệu cho bước này:
Kim loại chưa rõ1 nozzle head and nozzle
Dây nicrom1 nozzle heating coil
Vật liệu cách điện chưa rõ1 coil insulationCông cụ cần thiết:
Máy tiện kim loại4
4
Drive the screw
Drive the screw
Drive the screw through a gear from a motor, so its speed can be kept steady; 20 revolutions a minute in the example. Not given: the drive.
Vật liệu cho bước này:
Động cơ điện1 drive motor
Kim loại chưa rõ1 drive gearsCông cụ cần thiết:
Kích thước chưa rõ5
5
Extrude a rod
Extrude a rod
Keep the barrel 0 to 100 °F below the plastic's flow temperature and the nozzle 50 to 100 °F above it. Example: barrel at about 270 °F by steam, nozzle at about 400 °F, for a cellulose acetate with a flow temperature of 307 °F. Feed the hot, softened plastic into the throat at a steady rate. Carry the rod away on a conveyor and cool it at once with cold water, then cut it to length.
Công cụ cần thiết:
Nồi hơi
Hỏa kế
Nước làm mátVật liệu
5- 1 screwTạm thời
- 1 drive gearsTạm thời
- 1 nozzle heating coilTạm thời
- 1 coil insulationTạm thời
- 1 drive motorTạm thời
Vật liệu bản thiết kế liên kết
Bản thiết kế này làm ra
CC0 Phạm vi công cộng
Bản thiết kế này được phát hành theo CC0. Bạn tự do sao chép, sửa đổi, phân phối và sử dụng cho bất kỳ mục đích nào mà không cần xin phép.
Hỗ trợ nhà sáng tạo bằng cách mua sản phẩm qua bản thiết kế, nơi họ nhận Hoa hồng nhà sáng tạo do nhà bán hàng đặt, hoặc tạo phiên bản mới và kết nối trong bản thiết kế riêng để chia sẻ doanh thu.