Smith's Work Furnace of Rammed Clay With a Bellows Hole Through a Wooden Back (Theophilus, 12th Century)
The medieval workshop forge from Theophilus's De Diversis Artibus (12th century): a wooden back fixed in the ground by the wall with a finger-size bellows hole, a box of boards four fingers apart rammed two-thirds full of fresh-dug clay, then a hearth of clay and horse dung, pierced through the hole for the bellows tube. "In this manner compose all smith's furnaces."
Cơ bản
About 1 day plus drying
Hướng dẫn
1
1
His measures
His measures
Đang tải sổ tay Jupyter…
2
2
Read De Diversis Artibus, Book III
Read De Diversis Artibus, Book III
"Near the wall, by the window, on the left side of the person sitting, a piece of wood is fixed in the ground."
3
3
Set the wooden frame
Set the wooden frame
Fix a piece of wood firmly in the ground near the wall, three feet long and scarcely two fingers thick, with a finger-size hole through it four fingers above the ground. Peg on in front a straight piece four fingers wide and as long. In front of this fasten another of equal breadth and length so there is a space of four fingers between them, held outside by two or three stakes.
Vật liệu cho bước này:
Tấm gỗ cứng3 cái
Cọc gỗ3 cái
Thanh chốt gỗ1 cáiCông cụ cần thiết:
Cưa tay
Khoan tay quay và mũi khoan
Búa
Xẻng4
4
Ram the clay
Ram the clay
Take clay newly dug, not beaten nor mixed with water, put a little into the space and ram it hard with a rounded piece of wood, then more, until two parts of the space are filled and the third left empty. Take away the front wood, cut the clay level in front and on top with a long knife, and beat it hard with a thin piece of wood.
Vật liệu cho bước này:
Đất sét1 cáiCông cụ cần thiết:
Dao cắt da
Vồ gỗ5
5
Make the hearth
Make the hearth
Beat clay mixed with horse dung and make the furnace and its hearth, covering the wall so the fire cannot burn it. Pierce the clay with a slender stick through the hole in the back wood, for the bellows tube.
Vật liệu cho bước này:
Đất sét1 cái
Phân chuồng1 cáiCông cụ cần thiết:
Vồ gỗ
Xẻng6
6
Dry it
Dry it
Put the bellows tube in the hole, lay fire and charcoal at the back and front, and blow to dry the furnace.
Công cụ cần thiết:
Bễ thổi7
7
Troubleshooting
Troubleshooting
Furnace troubleshooting.
Flow
Loading...
8
8
History and honest limits
History and honest limits
From Theophilus, **De Diversis Artibus**, Book III, chapter III, translated by Robert Hendrie (1847) (checked on the archive.org scan essayuponvarious00hend, p. 211). The finger-to-centimetre figures, the tools and the diagram are ours.
Vật liệu
5- 3 cáiTạm thời
- 3 cáiTạm thời
- 1 cáiTạm thời
- 2 cáiTạm thời
- 1 cáiTạm thời
Bản thiết kế này làm ra
Blueprint liên quan
Các blueprint này chia sẻ kiến thức — kỹ thuật, vật liệu hoặc nguyên tắc
CC0 Phạm vi công cộng
Bản thiết kế này được phát hành theo CC0. Bạn tự do sao chép, sửa đổi, phân phối và sử dụng cho bất kỳ mục đích nào mà không cần xin phép.
Hỗ trợ nhà sáng tạo bằng cách mua sản phẩm qua bản thiết kế, nơi họ nhận Hoa hồng nhà sáng tạo do nhà bán hàng đặt, hoặc tạo phiên bản mới và kết nối trong bản thiết kế riêng để chia sẻ doanh thu.