Two-Part Epoxy Glue: Bis-Phenol Resin Thinned with Allyl Glycidyl Ether, Hardened with Diethylene Triamine
Woody

Yenziwe ngu-

Woody

18. uMfumfu 2026NO
7
0
0
0
0

Two-Part Epoxy Glue: Bis-Phenol Resin Thinned with Allyl Glycidyl Ether, Hardened with Diethylene Triamine

Bis-phenol epoxy resin is too thick to spread, so it is thinned with a fifth of its weight of allyl glycidyl ether, which joins the cure. That is part A; part B is diethylene triamine. Stir 10 parts of B into 100 of A, spread, join, and it hardens at room temperature: after six days at 25 °C, block joints held 3,550 lb/in² (Wiles and Newey, Shell, US 2,528,932, 1950). It bonds wood, metal and resins. The picture: our drawing of the two bottles and a glued joint.
Ophakathi
A week to full strength

Imiyalelo

1

Make part A

Warm 400 g bis-phenol epoxy resin until it flows (our step; it softens at 43 °C) and stir in 100 g allyl glycidyl ether, to a smooth, spreadable syrup. Bottle it.

Izinto zokwakha zalesi sinyathelo:

I-epoxy resin ye-bisphenolI-epoxy resin ye-bisphenol400 g
I-allyl glycidyl etherI-allyl glycidyl ether100 g

Amathuluzi adingekayo:

Ibhikha Le-borosilicateIbhikha Le-borosilicate
Ipuleti ElishisayoIpuleti Elishisayo
IsigovuziIsigovuzi
IthemomithaIthemomitha
Isikali Sedijithali SasekhishiniIsikali Sedijithali Sasekhishini
Amabhodlela engilazi anezivaloAmabhodlela engilazi anezivalo
Amagilavu erabhaAmagilavu erabha
2

Bottle part B

Bottle diethylene triamine separately and keep it closed: it is strongly alkaline and burns skin. You need 10 g for every 100 g of part A.

Izinto zokwakha zalesi sinyathelo:

I-diethylene triamineI-diethylene triamine50 g

Amathuluzi adingekayo:

Amabhodlela engilazi anezivaloAmabhodlela engilazi anezivalo
Amagilavu erabhaAmagilavu erabha
3

Mix only what you need

Weigh part A into a cup, add a tenth of its weight of part B, and stir well. It begins to cure at once, so mix just before gluing.

Amathuluzi adingekayo:

Inkomishi yokulinganisaInkomishi yokulinganisa
Isikali Sedijithali SasekhishiniIsikali Sedijithali Sasekhishini
IsigovuziIsigovuzi
Amagilavu erabhaAmagilavu erabha
4

Spread, join, wait

Spread a thin coat on both faces and press them together. At room temperature it sets in half an hour to a day and reaches full strength in one to two weeks; warmth speeds it up.

Amathuluzi adingekayo:

Ibhulashi legluIbhulashi leglu
5

Mixing table

Ilayisha incwadi ye-Jupyter…

Izinto

3

Amathuluzi Adingekayo

9

CC0 Isizinda Somphakathi

Le blueprint ikhishwe ngaphansi kwe-CC0. Ukhululekile ukukopisha, ukuguqula, ukusabalalisa, nokusebenzisa ngaphandle kwemvume.

Sekela uMenzi ngokuthenga imikhiqizo nge-Blueprint yabo IKhomishane Yomenzi kumiswe ngabathengisi, noma dala inguqulo entsha yale Blueprint bese uyifaka njengoxhumaniso ku-Blueprint yakho ukuze wabelane ngemali engenayo.

Ingxoxo

(0)

Ngena ukuze ujoyine ingxoxo

Kulayishwa amazwana...