Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Isopropanol
Philips' Ponjee and Verwijlen (US 4,639,382, 1987) made silver hold on acrylic by first dipping it in tannin dissolved in water mixed with an organic solvent; tannin in plain water gave no bond. This is their isopropanol solution: 50–85 % water, 15–50 % isopropanol by volume, 3.0–5.0 g tannin per litre, which gave full bonding in their cross-cut test. The sheet is then sensitised with weak stannous chloride and silvered by spraying the silver solution and the reducer together.
The picture: our diagram.
Intermediário
2 hours
Instruções
1
1
Dip in tannin solution for one minute
Dip in tannin solution for one minute
Make a solution of 3.0–5.0 g of tannic acid per litre in 50–85 % water and 15–50 % isopropanol by volume. Dip the acrylic sheet in it for one minute.
Materiais para este passo:
Chapa de acrílico1 peçaFerramentas necessárias:
Ácido tânico
Isopropanol
Água destilada
Tabuleiros de vidro
Proveta graduada
Balança de pratos
Hotte (com conduta)
Luvas de borracha2
2
Rinse with water
Rinse with water
Rinse the sheet with water.
Ferramentas necessárias:
Água destilada
Pisseta de laboratório3
3
Spray with stannous chloride for 12 seconds
Spray with stannous chloride for 12 seconds
Spray the face to be silvered with a solution of 0.1 g stannous chloride and 0.1 ml concentrated hydrochloric acid per litre of water, for 12 seconds. Rinse off the excess with water.
Ferramentas necessárias:
Cloreto estanoso
Ácido clorídrico
Água destilada
Pulverizador de água
Pisseta de laboratório
Óculos de proteção química
Luvas de borracha4
4
Spray silver and reducer together
Spray silver and reducer together
Atomise two solutions onto the face at the same time: silver nitrate with ammonia in water, and formalin in water. The patent gives no strengths: as required. Ours: a twin-nozzle spray gun.
Materiais para este passo:
Nitrato de Prata1 as requiredFerramentas necessárias:
Solução de amoníaco a 25-28 %
Solução de formaldeído (formol a 37 %)
Água destilada
Pistola de pulverização de dois bicos
Hotte (com conduta)
Óculos de proteção química
Luvas de borrachaMateriais
2- 1 peçaReferência
- 1 as requiredReferência
Ferramentas necessárias
16- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
Este projeto faz
Blueprints relacionados
Estes blueprints compartilham conhecimento — técnicas, materiais ou princípios
CC0 Domínio Público
Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.
Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.