Clamping Caul: Zinc Plate with a Pine Backing Board (Adamson, 1889)
Woody

Criado por

Woody

9. novembro 2026NO
4
0
0
0
0

Clamping Caul: Zinc Plate with a Pine Backing Board (Adamson, 1889)

A caul spreads clamping pressure evenly over glued work. D. Adamson (1889) prefers zinc for veneering cauls because it lasts longer than wood: a plate 1/8 to 1/4 in. thick (1/8 in. is enough), with a loose backing board of sound pine about 1 in. thick that keeps it flat and holds its heat. Only the zinc is warmed; the pine backing goes on cold. Source: D. Adamson, "Practical Veneering", Work, 5 October 1889, pp. 453-455.
Iniciante
Unknown

Instruções

1

Read Adamson

"Perhaps as a general thing the zinc is usually preferred of from 1/8 in. to 1/4 in. in thickness, the former being quite sufficient for ordinary purposes. ... Even with a zinc caul a backing of wood is necessary to keep it flat down to the work, and to prevent the heat from dispersing too rapidly."
2

Cut the zinc

Cut a zinc plate 1/8 in. thick (1/8 to 1/4 in. is usual; too thin does not hold the heat, thicker is only waste), large enough to cover the surface to be pressed and lying flat. Length and width are set by the work (not given). How it is cut is not given (ours: tin snips).

Materiais para este passo:

Chapa de zincoChapa de zinco1 1/8 in.

Ferramentas necessárias:

Tesoura de chapaTesoura de chapa
Dimensões desconhecidasDimensões desconhecidas
3

Make the backing board

Cut a backing board of good sound pine about 1 in. thick, the size of the zinc, and plane it flat so it keeps the zinc flat down to the work (ours: plane and straightedge).

Materiais para este passo:

Tábua de pinhoTábua de pinho1 about 1 in. thick

Ferramentas necessárias:

Serrote de marceneiroSerrote de marceneiro
Plaina manualPlaina manual
Régua de traçarRégua de traçar
4

Use it

Warm the zinc only (not so hot that it cannot be comfortably handled), lay it over the veneer with a sheet of slightly greased paper between, put the cold pine board on top, and screw down the hand-screws evenly until the glue oozes out at the edges. Leave it until the zinc is cold, an hour or two.

Ferramentas necessárias:

GramposGrampos

Materiais

2

Ferramentas necessárias

6

CC0 Domínio Público

Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.

Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.

Discussão

(0)

Entrar para participar da discussão

Carregando comentários...