Helium: Uraninite Heated with Dilute Sulphuric Acid, Purified through Hot Quartz (Thorpe 1912)
Perigoso
Charlie

Criado por

Charlie

1. novembro 2026DE
5
0
0
0
0

Helium: Uraninite Heated with Dilute Sulphuric Acid, Purified through Hot Quartz (Thorpe 1912)

Uranium minerals hold helium trapped inside them. Heating the powder with dilute sulphuric acid lets all of it out. Fused quartz at 1000–1200 °C lets helium through and nothing else, so the helium comes out pure. Result: helium free from nitrogen and the other inert gases. For comparison, 1 g of cleveite (a kind of uraninite) gives over 3.2 cc. Source: Thorpe, Dictionary of Applied Chemistry vol. 3 (1912), p. 34, after Travers and after Jacquerod and Perrot. Not given: acid strength, amounts, yield from plain uraninite. Uraninite is radioactive. Picture drawn by Youblob.
Avançado
1 day

Conteúdo perigoso

Este blueprint contém procedimentos perigosos. Faça login e ative o conteúdo perigoso nas configurações da sua conta para ver as instruções passo a passo.

Entrar

CC0 Domínio Público

Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.

Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.

Discussão

(0)

Entrar para participar da discussão

Carregando comentários...