LDPE Pellets: Ethylene Polymerised at 1500 Atmospheres with a Trace of Oxygen
Perigoso
Charlie

Criado por

Charlie

19. outubro 2026DE
14
0
0
2
0

LDPE Pellets: Ethylene Polymerised at 1500 Atmospheres with a Trace of Oxygen

Polyethylene was discovered at ICI by Fawcett, Gibson and Perrin (US 2,153,553, 1939): ethylene squeezed to over a thousand atmospheres and heated, with a trace of oxygen to start the reaction, turns into a tough, waxy solid that melts at about 120 °C. Their Example III, at 1500 atmospheres and 210 °C for 5 hours, turned 80 % of the ethylene into polymer. The heat of reaction must be carried away, or the gas decomposes explosively. Extruding it into pellets is our step. The picture: our diagram.
Avançado
About 6 hours

Conteúdo perigoso

Este blueprint contém procedimentos perigosos. Faça login e ative o conteúdo perigoso nas configurações da sua conta para ver as instruções passo a passo.

Entrar

Blueprints relacionados

Estes blueprints compartilham conhecimento — técnicas, materiais ou princípios

CC0 Domínio Público

Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.

Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.

Discussão

(0)

Entrar para participar da discussão

Carregando comentários...