Rasps and Files for Wood: Why the Teeth Are Completely Different
Take a metalworking file to a piece of wood and it will clog solid in about four strokes. The teeth are far too close together for a wood chip, which is bulky and fibrous where a metal chip is a tiny curl.
So wood gets a RASP: individually punched teeth, widely spaced, each standing alone with an enormous open space around it. It tears rather than cuts, leaves a rough surface, and removes wood astonishingly fast.
Between the two sits the cabinet rasp and the wood file, and knowing which to reach for at which stage is most of the skill. This rung also covers the one thing all of them share: work with the grain, or you tear it.
Iniciante
3 hours
Instruções
1
1
Compare the teeth side by side
Compare the teeth side by side
Lay a metal file and a rasp next to each other under a loupe. The file has continuous rows a fraction of a millimetre apart; the rasp has individual raised points several millimetres apart, each punched up out of the surface.
That spacing is the whole design. A wood shaving is bulky, springy and does not break up, so it needs somewhere to go — and a rasp gives each tooth a gullet many times the size of the chip. A metal file gives it almost nothing, which is why wood packs it solid immediately.
The corollary is that a rasp is useless on metal: the widely spaced points dig in, chatter, and chip themselves. The two tools genuinely cannot be swapped, and this is not a matter of quality or coarseness.
Ferramentas necessárias:
Grosa
Lima para metal
Lupa de joalheiro2
2
The progression: rasp, cabinet rasp, file, abrasive
The progression: rasp, cabinet rasp, file, abrasive
Start with a coarse rasp to get the shape, move to a fine or cabinet rasp to remove the worst of the tearing, then a wood file to take out the rasp marks, then abrasive paper.
Each stage exists to remove the damage left by the previous one, exactly as the sharpening grit progression does — and skipping a stage costs time for the same reason, because the finer tool has to work through deeper marks at its own much slower rate.
The coarse rasp does the shaping and should be used boldly; everything after it is repair work. Spending a long time with a coarse rasp trying to be delicate is the wrong way round — shape fast, then change tool.
Materiais para este passo:
Tábua de madeira de lei1 peça
Sortido de lixa1 peçaFerramentas necessárias:
Grosa
Grosa para madeira
Limas de mão3
3
Work with the grain, and support the fibres
Work with the grain, and support the fibres
Push the rasp diagonally across the work but angled so it travels WITH the grain rather than against it. Against the grain, the teeth lift fibres and tear out chunks below the surface you are cutting.
Around a curve the grain direction changes as you go, so the correct stroke direction changes with it. Where the grain runs downhill into the cut, you are with it; where it runs uphill, reverse and come at that part from the other side. Watch the surface: tearing is immediately visible as a rough torn patch rather than a cleanly abraded one.
End grain tears worst of all. Back it with a scrap block clamped tight against the exit side, so the fibres at the edge are supported and cannot break away — the same trick that stops a drill bit blowing out the back of a hole.
Materiais para este passo:
Tábua de madeira de lei1 peça
Tábua de resinosa seca1 peçaFerramentas necessárias:
Grosa
Torno de bancada pesado4
4
Keep them clear — wood clogs worse than metal
Keep them clear — wood clogs worse than metal
Resinous softwood packs a rasp faster than aluminium packs a file, and a clogged rasp burnishes the wood instead of cutting it, which looks like the tool has gone blunt.
Clear it with a file card the same way, brushing along the rows. For a rasp, the points are individual so the direction matters less, but packed resin needs more than a brush — a stiff bristle brush and hot soapy water, dried immediately, or a wipe with solvent.
Rasps are also far more forgiving to store than files, but the same rule applies: a rasp whose points have been knocked flat against another tool leaves scratches it cannot be persuaded out of. Hang them, keep them dry, and a good rasp will outlast several generations of abrasive paper.
Ferramentas necessárias:
Escova para limas
Grosa
Grosa para madeira
Pano de algodãoMateriais
3- 1 peçaReferência
- 1 peçaReferência
- 1 peçaReferência
Ferramentas necessárias
8- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
Blueprints relacionados
Estes blueprints compartilham conhecimento — técnicas, materiais ou princípios
CC0 Domínio Público
Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.
Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.