Splitting and Seasoning Firewood
Freshly cut wood can be up to half water by weight, and a fire burning it spends its heat boiling that water off, with smoke and tar in the chimney. Firewood is ready below 20 % moisture. Splitting opens the wood so it dries, and a stack in sun and wind does the rest: softwoods take about 6 to 12 months, hardwoods such as oak and beech 12 to 24.
Test a freshly split face with a moisture meter, never the weathered outside.
Iniciante
1 day of work, 6–24 months drying
Instruções
1
1
Saw to length
Saw to length
Measure your firebox and saw the logs into rounds about 5 cm shorter than it. Keep one wide, flat round as a chopping block.
Materiais para este passo:
Toros de folhosa (carvalho, ácer, faia)500 kgFerramentas necessárias:
Serra traçadeira
Fita métrica2
2
Split on the block
Split on the block
Stand a round on the block, bark side out of any crack. Feet apart, swing the splitting axe down into the crack or across the centre. Split rounds into pieces about 8–15 cm across.
Ferramentas necessárias:
Machado de rachar
Óculos de segurança
Botas de segurança com biqueira de aço
Luvas de trabalho em couro3
3
Wedge the stubborn ones
Wedge the stubborn ones
For knotty rounds, tap a steel wedge into a crack and drive it with the sledgehammer; add a second wedge along the crack if the first sticks.
Ferramentas necessárias:
Conjunto de cunhas de aço
Marreta
Óculos de segurança4
4
Stack off the ground
Stack off the ground
Lay pallets in a sunny, windy spot. Stack the splits in single rows with gaps between them, ends criss-crossed at each end of the row to hold it up.
Ferramentas necessárias:
Palete de madeira5
5
Cover the top only
Cover the top only
Lay a tarp over the top of the stack and weigh it down; leave the sides open so the wind can carry the moisture away.
Ferramentas necessárias:
Lona6
6
Test before you burn
Test before you burn
After 6 months for softwood or 12 for hardwood, split a piece from the middle of the stack and push the meter's pins into the fresh face. Below 20 % it is ready; if not, test again in a month.
Ferramentas necessárias:
Medidor de humidade
Machado de rachar7
7
Troubleshooting
Troubleshooting
Firewood troubleshooting.
Flow
Loading...
Materiais
1- Referência
Ferramentas necessárias
11- Referência
- 1 vendor sell this, none ship to you yetReferência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
- Referência
Este projeto faz
Blueprints relacionados
Estes blueprints compartilham conhecimento — técnicas, materiais ou princípios
CC0 Domínio Público
Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.
Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.