Colaboración
ARTE
BELLEZA Y BIENESTAR
ARTESANÍA
CULTURA E HISTORIA
ENTRETENIMIENTO
MEDIO AMBIENTE
COMIDA Y BEBIDAS
INGENIERÍA INVERSA
CIENCIAS
DEPORTES
TECNOLOGÍA
TECNOLOGÍA VESTIBLE
Angled-Side Spade Bits: Each Wing Bent Forwards Along a Diagonal Line, the Way the Bit Turns (Vasudeva, 2005)
Forge

Creado por

Forge

13. noviembre 2026NO
0
0
0
0
0

Angled-Side Spade Bits: Each Wing Bent Forwards Along a Diagonal Line, the Way the Bit Turns (Vasudeva, 2005)

Kailash C. Vasudeva of Waterloo, Canada, received US 6,957,937, dated 25 October 2005, for Maxtech Manufacturing. Both outer wings of the blade are bent forwards, the way the bit turns. Each bends along a line from low on the side to a point on the cutting edge a little over halfway out. The outer ends of the cutting edge then lead, with a spur at each. The chips change direction where they cross the bend and break up, and come out of the hole more easily. We forge 16, 20 and 25 mm bits and bend the wings hot. The patent gives no bend angle or sizes; ours are 10 degrees and the sizes shown.
Avanzado
About 1 day

Instrucciones

1

How far the bend brings the corners forward

Cargando el cuaderno de Jupyter…
2

Read US 6,957,937

"The longitudinal sides of the head portion are bent along a bend 9, in the direction of rotation of the spade drill bit during operation, so that the outer ends of the cutting edge are bent forwards in the rotating direction." "The shorter the bend 9, the larger the angle with the longitudinal direction is going to be, and the more abrupt is the chip break-up. Larger angles require more power for drilling."
3

Forge the blades

Cut three 170 mm lengths of 10 mm octagonal tool steel. Heat 50 mm of one end to a bright orange in the forge and flatten it on the anvil to about 3 mm thick, centred on the bar. Hammer across it with the peen to spread it wider than the bit, about 2 mm over its size: 18, 22 and 27 mm. Draw the neck down smoothly where the blade meets the bar and keep the blade in line with it. Reheat as soon as the colour fades to red. Finally heat each one to a cherry red and let it cool slowly in the air, to soften it for filing.

Materiales para este paso:

Barra octogonal de acero para herramientasBarra octogonal de acero para herramientas3 piezas

Herramientas necesarias:

Sierra para metalesSierra para metales
Tornillo de bancoTornillo de banco
FraguaFragua
YunqueYunque
Martillo de forjaMartillo de forja
Tenazas de fraguaTenazas de fragua
Guantes de soldadorGuantes de soldador
Gafas de seguridadGafas de seguridad
4

Print the template

Full-size A4 template: the outlines of the 16, 20 and 25 mm bits with straight cutting edges and spurs, the two bend lines and the hanging hole. Print at 100 %; its 50 mm bar must measure 50 mm.
Archivo de DisenoPDFCC0 - Free
5

Grind the outline

Glue each bit's outline from the template on its blade, centred on the bar. Grind to the lines on the bench grinder, dipping the steel in water often: the two sides parallel, the shoulders square across, the point in the middle. Grind the blade's two faces flat and parallel to 2.5 mm. Grind three flats on the end of the shank, a third of the way round from each other, 20 mm long, for the chuck's jaws. Leave a spur 2 mm wide and 2 mm high at each outer end of the cutting edges. Scribe the two bend lines through the paper onto both faces. Drill a 3 mm hole at the template's circle.

Herramientas necesarias:

Impresora de inyección de tintaImpresora de inyección de tinta
ColaCola
Esmeril de bancoEsmeril de banco
Cubo de templeCubo de temple
AguaAgua
Juego de limasJuego de limas
Tornillo de bancoTornillo de banco
Calibre digital de 6 pulgadasCalibre digital de 6 pulgadas
Gafas de seguridadGafas de seguridad
6

Bend the wings

Heat the blade to a bright red. Grip it in the vice with one bend line exactly along the top of the jaws and the wing standing above them. With the face towards you and the point up, push the left wing towards you about 10 degrees with the flat-nose pliers or light hammer blows close to the jaws, so it bends on the line. Reheat, grip along the other line and push the right wing away from you the same amount. Look down the bit from the point: the two wings should lean opposite ways, like a shallow S, as in his Fig. 2D. Let it cool slowly in the air.

Herramientas necesarias:

FraguaFragua
Tenazas de fraguaTenazas de fragua
Tornillo de bancoTornillo de banco
Martillo de forjaMartillo de forja
Alicates de boca planaAlicates de boca plana
Guantes de soldadorGuantes de soldador
Gafas de seguridadGafas de seguridad
7

Grind the cutting edges

Bevel each cutting edge and each side of the blade so the edge that leads as the bit turns is sharp and the face behind it clears the wood. Sharpen the spurs' outer edges and the point's two leading edges the same way.

Herramientas necesarias:

Esmeril de bancoEsmeril de banco
Cubo de templeCubo de temple
AguaAgua
Juego de limasJuego de limas
Tornillo de bancoTornillo de banco
8

Harden and temper

Heat the blade and the neck evenly to a cherry red, until a magnet no longer sticks to it, and quench it straight down in water, moving it up and down. Rub the faces bright with a stone. Heat the shank gently 30 mm behind the blade and watch the colours run down; quench again as soon as a dark straw colour reaches the shoulders and the point. Do the other two.

Herramientas necesarias:

FraguaFragua
Tenazas de fraguaTenazas de fragua
Imán pequeñoImán pequeño
Cubo de templeCubo de temple
AguaAgua
Piedra de afilarPiedra de afilar
Guantes de soldadorGuantes de soldador
Gafas de seguridadGafas de seguridad
9

Sharpen and test

Hone the cutting edges on the shoulders and the point with the stone, keeping their angles, and take the burr off. Chuck a bit by its flats and bore a scrap of hardwood: it should start on the point without wandering, cut two clean shavings from the shoulders and leave a round hole of its own size; check it with the caliper.

Herramientas necesarias:

Piedra de afilarPiedra de afilar
Taladro inalámbricoTaladro inalámbrico
Tabla de madera duraTabla de madera dura
Calibre digital de 6 pulgadasCalibre digital de 6 pulgadas
Gafas de seguridadGafas de seguridad
10

Troubleshooting

Spade bit troubleshooting.

Flow

Loading...
11

History and honest limits

**Kailash C. Vasudeva** of Waterloo, Canada, assignor to Maxtech Manufacturing Inc., US 6,957,937 B2, dated 25 October 2005, filed 20 February 2002. His head's sides are "bent along a bend 9, in the direction of rotation", the bend running from a position on the side nearer the bottom of the head to a position on the cutting edge between its outer end and the tip. He shows arced and straight cutting edges, serrated sides, chip-breaking reliefs on the tip, and a head made separately by powder metallurgy. We build the straight-edged form of his Figs. 2E to 2G with spurs, forged in one piece, without the reliefs. He gives no bend angle or sizes; 10 degrees and our sizes are ours, the bend line placed as measured off his Fig. 2B.

Materiales

1

Herramientas requeridas

20

Archivos de diseño

1

CC0 Dominio público

Este Blueprint se publica bajo CC0. Eres libre de copiar, modificar, distribuir y usar este trabajo para cualquier propósito, sin pedir permiso.

Apoya al Maker comprando productos a través de su Blueprint, donde gana una Comisión del Maker establecida por los vendedores, o crea una nueva iteración de este Blueprint e inclúyela como conexión en tu propio Blueprint para compartir ingresos.

Discusión

(0)

Iniciar sesión para unirte a la discusión

Cargando comentarios...