Brick Smith's Hearth: Stone Base, Firebrick Top in an Iron Rim, a Cannon-Shot Tuyere and a Slake Trough (Edwinson, 1886)
Forge

Dibuat oleh

Forge

14. November 2026NO
7
0
0
0
0

Brick Smith's Hearth: Stone Base, Firebrick Top in an Iron Rim, a Cannon-Shot Tuyere and a Slake Trough (Edwinson, 1886)

The fixed smith's hearth George Edwinson told Amateur Work readers to build (1886): stone below, firebrick in fireclay on top, every course bound with hoop iron, a 4 in. iron rim forming the hearth pan, a fire back and tuyere made from a 1 in. plate and a bored 14-pounder iron shot, a slanting flue, a 10 x 10 x 22 in. slake trough, and a clinker floor.
Menengah
Two to three days of building

Instruksi

1

His sizes

Memuat notebook Jupyter…
2

Read Edwinson

"The foundation of this structure up to within one foot of the top may be of stone, but the finishing courses should be of firebrick."
3

Build the base

Build the hearth in stone up to 1 ft (30 cm) below the top, binding every course with pieces of hoop iron. Leave an arch at the back for the coal pit and the blast pipe (figs. 4, 5). Overall size is ours: fit it to your shop.

Material untuk langkah ini:

Balok batuBalok batu1 buah
Simpai besiSimpai besi1 buah
Tanah Liat Tahan ApiTanah Liat Tahan Api1 buah

Alat yang dibutuhkan:

Sendok semenSendok semen
WaterpasWaterpas
4

Make the fire back and tuyere

Bore a 3/4 in. hole through a 14-pounder iron shot and open it to a 1 in. taper on one side. Cut and countersink a hole in a 1 in. iron plate to take a third of the shot, and drill four 1/2 in. holes to bolt the plate through the wall with nuts and fish plates. (Or buy a fire back and tue-iron.)

Material untuk langkah ini:

Gotri besi (pemberat)Gotri besi (pemberat)1 buah
Pelat besiPelat besi1 buah
Aneka baut segi enamAneka baut segi enam1 buah

Alat yang dibutuhkan:

Mesin Bor DudukMesin Bor Duduk
Perapian pandai besiPerapian pandai besi
PaluPalu
5

Firebrick top and back

Lay the top courses and the back wall round the tuyere in firebrick bedded and jointed with fireclay, still binding each course with hoop iron. Build in the fire back with the shot as the tuyere, and leave a slanting flue hole just above it (fig. 5).

Material untuk langkah ini:

Bata Tahan ApiBata Tahan Api1 buah
Tanah Liat Tahan ApiTanah Liat Tahan Api1 buah
Simpai besiSimpai besi1 buah

Alat yang dibutuhkan:

Sendok semenSendok semen
WaterpasWaterpas
6

Fit the slake trough

Before the last course, set in a water trough 10 in. deep and wide and 22 in. long, of sheet iron, cast iron or stone, inside the rim line; bolt a sheet-iron one to the rim. A sheet-iron division riveted across gives a coal trough too.

Material untuk langkah ini:

Pelat Baja LunakPelat Baja Lunak1 buah
Paku keling besiPaku keling besi1 buah
AirAir1 buah

Alat yang dibutuhkan:

Mesin Bor DudukMesin Bor Duduk
PaluPalu
7

Bind with the rim

Bind the top course with a rim of 1/4 x 4 in. iron, half below the brick edge and half above it to make the hearth pan, its ends bolted to the back wall with 3/8 in. bolts built into the brickwork.

Material untuk langkah ini:

Pelat besiPelat besi1 buah
Aneka baut segi enamAneka baut segi enam1 buah

Alat yang dibutuhkan:

Perapian pandai besiPerapian pandai besi
Landasan TempaLandasan Tempa
PaluPalu
Mesin Bor DudukMesin Bor Duduk
8

Connect the blast

Bring the pipe from a fan or bellows under the arch to the back of the tue-iron. He reckons about 150 cu ft (4.2 m3) of air a minute for a welding heat: a 9 in. fan at about 360 rpm or a double-action bellows.

Alat yang dibutuhkan:

Peniup udaraPeniup udara
9

Lay the floor

Ram wetted smiths', foundry or boiler clinkers sprinkled with a little Portland cement hard and level, with a thin layer of smithy cinder ashes beaten on top. Stone or ordinary concrete floors misbehave when hot iron is dropped on them.

Material untuk langkah ini:

Semen portlandSemen portland1 buah
AirAir1 buah

Alat yang dibutuhkan:

PaluPalu
10

Troubleshooting

Hearth troubleshooting.

Flow

Loading...
11

History and honest limits

From George Edwinson, "Smithing and Forging" I, **Amateur Work, Illustrated**, vol. V (1886), pp. 161-162 and figs. 2, 4, 5 (checked on the archive.org scan amateurworkillus05lond). He gives no overall hearth size; that and the metric figures and tools are ours.

Bahan

11

Alat yang Diperlukan

7

Cetak biru ini membuat

CC0 Domain Publik

Cetak biru ini dirilis di bawah CC0. Anda bebas untuk menyalin, memodifikasi, mendistribusikan, dan menggunakan karya ini untuk tujuan apa pun, termasuk komersial, tanpa meminta izin.

Dukung Maker dengan membeli produk melalui Cetak Biru mereka di mana mereka mendapatkan Komisi Pembuat yang ditetapkan oleh Penjual, atau buat iterasi baru dari Cetak Biru ini dan masukkan sebagai koneksi di milik Anda sendiri.

Diskusi

(0)

Masuk untuk bergabung dengan diskusi

Memuat komentar...