Thulium: Oxide Reduced with Aluminium in Flowing Argon and the Vapour Condensed (CN 104152695 B)
Pellets of thulium oxide and aluminium are fed into an induction furnace at 1700 °C. The aluminium takes the oxygen and stays behind as slag. Thulium boils off as vapour, and a stream of argon carries it into a water-cooled tank where it condenses to metal.
Result: thulium metal, 99.5 % of the thulium recovered. No vacuum pump is needed: the moving argon sweeps the vapour away as fast as it forms.
Source: Zhang, Dou et al. (Northeastern University), Chinese patent CN 104152695 B (2014), Example 1. Not given: batch size, the form of the aluminium, pellet size, the purity of the thulium. Picture: Wikimedia Commons.
उन्नत
1 day
निर्देश
1
1
Weigh and mix
Weigh and mix
Weigh thulium oxide and aluminium, both over 99.0 % pure, in the molar ratio 1 : 2.2: 10 % more aluminium than the reaction needs (ours: about 15.4 g of aluminium to 100 g of oxide). Mix them evenly.
इस चरण के लिए सामग्री:
थुलियम ऑक्साइड100 ग्राआवश्यक उपकरण:
ऐलुमिनियम
तौल का काँटा2
2
Press into pellets
Press into pellets
Press the mix in a roller press at 100 kg/cm² into lumpy pellets.
आवश्यक उपकरण:
रोलर प्रेस3
3
Reduce in flowing argon
Reduce in flowing argon
Run argon (99.95 %) through a medium-frequency induction furnace (the patent's coil is 220 mm across) at 5 L/min; ours: set the flow with a rotameter. Feed the pellets in continuously and hold them at 1700 °C for 30 min. The thulium leaves as vapour mixed with the argon; draw the slag off continuously.
आवश्यक उपकरण:
प्रेरण भट्ठी
आर्गन
रोटामीटर4
4
Condense the thulium
Condense the thulium
Let the argon carry the vapour out of the furnace through a sealed pipe straight into a condensing tank cooled by circulating water. The thulium condenses there as metal: 99.5 % recovered. Example 2 of the patent runs at 1500 °C for 60 min with 15 L/min of argon (pellets pressed at 150 kg/cm²) and reports 99.2 %.
आवश्यक उपकरण:
संघनन कक्ष
शीतलन जलसामग्री
1- 100 ग्राप्लेसहोल्डर
यह ब्लूप्रिंट बनाता है
संबंधित ब्लूप्रिंट
ये ब्लूप्रिंट ज्ञान साझा करते हैं — तकनीक, सामग्री या सिद्धांत

खतरनाक
Erbium, Ytterbium, Thulium and Lutetium Oxides: Xenotime Separated on Ion Exchange Columns with EDTA and HEDTA (Spedding and Powell, US 2,956,858)
Charlie द्वारा
अकार्बनिक
2
0
0
0
0
0

खतरनाक
Aluminium by Hall–Héroult Electrolysis: Alumina in Molten Cryolite
Forge द्वारा
धातु का काम
6
0
0
0
0
0

Argon: Air Led over Calcium Carbide and Calcium Chloride at 800 °C (Fischer and Ringe, Thorpe 1912)
Charlie द्वारा
अकार्बनिक
0
0
0
0
0
0

Ytterbium: Oxide Reduced by Lanthanum at 1020 °C in Vacuum, Metal Distilled Off (Shindo and Yagi, US 2010/0260640)
Charlie द्वारा
अकार्बनिक
1
0
0
0
0
0
CC0 पब्लिक डोमेन
यह ब्लूप्रिंट CC0 के तहत जारी किया गया है। आप बिना अनुमति माँगे इस कार्य को किसी भी उद्देश्य के लिए कॉपी, संशोधित, वितरित और उपयोग करने के लिए स्वतंत्र हैं।
उनके ब्लूप्रिंट के माध्यम से उत्पाद खरीदकर मेकर का समर्थन करें जहाँ वे मेकर कमीशन कमाते हैं जो विक्रेताओं द्वारा निर्धारित होता है, या इस ब्लूप्रिंट का नया संस्करण बनाएँ और राजस्व साझा करने के लिए इसे अपने ब्लूप्रिंट में कनेक्शन के रूप में शामिल करें।