Smith's Fire Rake (Poker): a 3/8 in. Rod Drawn to a Flat Point, Crooked, and Looped Over the Anvil (Edwinson, 1886)
The first job George Edwinson set his readers in Amateur Work (1886): the smith's rake for the forge fire, which "might be dubbed a poker". A yard of 3/8 in. iron rod drawn to a square then flat point with quarter turns, bent into a crook, and the other end bent round in three heats into a loop handle.
ចាប់ផ្តើម
An hour at the forge
ការណែនាំ
1
1
His sizes
His sizes
កំពុងផ្ទុកសៀវភៅ Jupyter…
2
2
Read Edwinson
Read Edwinson
"The rake, Fig. 16, might be dubbed a poker, and as this is the most simple tool, we will deal with that first."
3
3
Light a small fire
Light a small fire
Pile slack round the tuyere, scoop a shallow pit in front of it, put in shavings with a few cinders on top, light and blow gently. Draw slack in until the heap glows, then damp the outside so the fire stays within 6 in. (15 cm) of the tuyere.
សម្ភារៈសម្រាប់ជំហាននេះ៖
ធ្យូងថ្មប៊ីទុយមេន1 ដុំឧបករណ៍ដែលត្រូវការ៖
ឡជាងដែក4
4
Draw the point
Draw the point
Cut 36 in. (91 cm) of 3/8 in. (10 mm) iron rod with a cold chisel. Heat 2 in. of one end glowing white. On the outer edge of the anvil, hammer it lightly on the tip, giving the rod a quarter turn after each blow and drawing it back, to a square point. Strike only while it glows; reheat at a dull red. Next heat, round the corners and draw a flat tapering point (fig. 17).
សម្ភារៈសម្រាប់ជំហាននេះ៖
ដំបងដែកវាយ1 ដុំឧបករណ៍ដែលត្រូវការ៖
ផ្លុងកាត់ដែកត្រជាក់
ឡជាងដែក
ទាំងជល់ (កំណាត់ដែក)
ញញួរ5
5
Crook the end
Crook the end
Heat the point to a dull red and bend it over the outer edge of the anvil with a few light blows into the crook (fig. 16).
ឧបករណ៍ដែលត្រូវការ៖
ឡជាងដែក
ទាំងជល់ (កំណាត់ដែក)
ញញួរ6
6
Bend the loop
Bend the loop
Heat the rod about 10 in. from the other end to redness and bend it over the anvil edge (fig. 18). Heat 3 in. more of the bent part and shape it (fig. 19). Heat again and bring the end round to touch the shoulder (fig. 20), then shape the loop hot with light blows. (Experienced smiths scarf the end and weld it to the shoulder.)
ឧបករណ៍ដែលត្រូវការ៖
ឡជាងដែក
ទាំងជល់ (កំណាត់ដែក)
ញញួរ7
7
Troubleshooting
Troubleshooting
Rake troubleshooting.
Flow
Loading...
8
8
History and honest limits
History and honest limits
From George Edwinson, "Smithing and Forging" II, **Amateur Work, Illustrated**, vol. V (1886), pp. 211-213 and figs. 15-20 (checked on the archive.org scan amateurworkillus05lond). Metric figures and the tools are ours.
សម្ភារៈ
2- 1 ដុំកន្លែងទុក
- 1 ដុំកន្លែងទុក
ប្លង់ពាក់ព័ន្ធ
ប្លង់ទាំងនេះចែករំលែកចំណេះដឹង — បច្ចេកទេស សម្ភារៈ ឬគោលការណ៍
CC0 សាធារណៈ
ប្លង់នេះត្រូវបានចេញផ្សាយក្រោម CC0។ អ្នកមានសិទ្ធិចម្លង កែប្រែ ចែកចាយ និងប្រើប្រាស់ដោយមិនចាំបាច់សុំអនុញ្ញាត។
គាំទ្រអ្នកបង្កើតដោយទិញផលិតផលតាមរយៈប្លង់របស់ពួកគេ ដែលពួកគេទទួលបាន កម្រៃជើងសារអ្នកបង្កើត កំណត់ដោយអ្នកលក់ ឬបង្កើតកំណែថ្មីនៃប្លង់នេះ ហើយបញ្ចូលជាការតភ្ជាប់ក្នុងប្លង់របស់អ្នកដើម្បីចែករំលែកចំណូល។