PTFE Disc: Sintered in a Molten Nitrate Bath, Cooled Slowly (Brubaker & Hanford 1946)

A PTFE disc pressed cold, then sintered by dipping it in molten salt at 380 °C for half an hour. Instead of being quenched, it cools slowly between magnesite blocks. The patent says slowly cooled pieces are a little softer and less stiff, which is often better for machining. Source: M. M. Brubaker and W. E. Hanford (du Pont), US 2,400,099 (1946), Example II. The patent gives no nitrate-to-nitrite ratio. The mould, press, pot and burner are ours. Picture drawn by Youblob.
고급
1 day

안내

1

Press a disc at 500 psi

At 25 °C, press PTFE powder at 500 lb/sq in into a disc 2 in across and ⅜ in thick.

이 단계의 재료:

PTFE 수지 분말PTFE 수지 분말1 as required for the disc

필요한 도구:

압축 성형 금형압축 성형 금형
유압 프레스유압 프레스
자자
2

Melt the salt bath at 380 °C

Melt a mixture of sodium nitrate and sodium nitrite and hold it at 380 °C. The patent gives no ratio. Ours: a cast iron pot on a gas burner.

필요한 도구:

칠레 초석(질산나트륨)칠레 초석(질산나트륨)
아질산나트륨아질산나트륨
무쇠 솥무쇠 솥
가스 버너가스 버너
표시기 달린 열전대표시기 달린 열전대
3

Dip the disc for half an hour

Lower the pressed disc into the molten bath and leave it there for ½ hour.

필요한 도구:

부집게부집게
무쇠 솥무쇠 솥
표시기 달린 열전대표시기 달린 열전대
4

Cool it slowly between magnesite blocks

Take the disc out and lay it between two magnesite blocks so it cools to room temperature over 1 hour. It comes out tough and even, close to its pressed shape.

필요한 도구:

부집게부집게
마그네사이트 블록마그네사이트 블록

재료

1
  • 1 as required for the disc
    플레이스홀더

필요 도구

10

이 블루프린트로 만드는 것

CC0 퍼블릭 도메인

이 블루프린트는 CC0로 공개되었습니다. 어떤 목적으로든 자유롭게 복사, 수정, 배포 및 사용할 수 있습니다.

제품 구매를 통해 메이커를 지원하세요. 판매자가 설정한 메이커 커미션 을 받거나, 이 블루프린트의 새로운 반복을 만들어 연결로 포함시킬 수 있습니다.

토론

(0)

로그인 하여 토론에 참여하세요

댓글 로딩 중...