BlueprintCulture And HistoryEraIndustry 3.0 — Assembly Line & Mass Production (1913)

Industry 3.0 — Assembly Line & Mass Production (1913)

327 blueprint tersedia

Blueprint (327)

Ferrite Toroid Core: Copper-Cadmium Ferrite, 200-Hour Grind, 1000 °C in Oxygen (Snoek 1948, Ex. I)
Berbahaya

Ferrite Toroid Core: Copper-Cadmium Ferrite, 200-Hour Grind, 1000 °C in Oxygen (Snoek 1948, Ex. I)

oleh CharlieDE

Organik

16
0
0
0
0
0
Extruded Polystyrene Foam: Butylene-Blown Logs 20 Inches Across (McIntire, Dow 1948, Ex. 4)

Extruded Polystyrene Foam: Butylene-Blown Logs 20 Inches Across (McIntire, Dow 1948, Ex. 4)

oleh CharlieDE

Organik

9
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 75 °C (McIntire, Dow 1948, Ex. 3, Test 4)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 75 °C (McIntire, Dow 1948, Ex. 3, Test 4)

oleh CharlieDE

Organik

8
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 60 °C (McIntire, Dow 1948, Ex. 3, Test 3)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 60 °C (McIntire, Dow 1948, Ex. 3, Test 3)

oleh CharlieDE

Organik

10
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 50 °C (McIntire, Dow 1948, Ex. 3, Test 2)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 50 °C (McIntire, Dow 1948, Ex. 3, Test 2)

oleh CharlieDE

Organik

8
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 40 °C (McIntire, Dow 1948, Ex. 3, Test 1)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 40 °C (McIntire, Dow 1948, Ex. 3, Test 1)

oleh CharlieDE

Industry 3.0 — Assembly Line & Mass Production (1913)

9
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 100 °C (McIntire, Dow 1948, Ex. 2)
Berbahaya

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 100 °C (McIntire, Dow 1948, Ex. 2)

oleh CharlieDE

Organik

12
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)
Berbahaya

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)

oleh CharlieDE

Organik

11
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 80 °C (McIntire, Dow 1948, Ex. 2)
Berbahaya

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 80 °C (McIntire, Dow 1948, Ex. 2)

oleh CharlieDE

Organik

13
0
0
0
0
0
Ferrite Toroid Core: Nickel-Zinc Ferrite, Then 3 Days at 950 °C in Oxygen (Snoek 1948, Ex. III)
Berbahaya

Ferrite Toroid Core: Nickel-Zinc Ferrite, Then 3 Days at 950 °C in Oxygen (Snoek 1948, Ex. III)

oleh CharlieDE

Bahan

3
0
0
0
0
0
Ferrite Toroid Core: Magnesium-Zinc Ferrite, One-Day Grind, 1400 °C (Snoek 1948, Ex. II)

Ferrite Toroid Core: Magnesium-Zinc Ferrite, One-Day Grind, 1400 °C (Snoek 1948, Ex. II)

oleh CharlieDE

Bahan

3
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

4
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

6
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

4
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1250 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

1
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

1
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

7
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1200 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

2
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

3
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

5
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1150 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

6
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Three Times at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

4
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Twice at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

4
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

Ferrite Toroid Core: Copper-Zinc Ferrite Sintered at 1100 °C, Presintered Once at 900 °C (Snoek 1948, Ex. I)

oleh CharlieDE

Bahan

1
0
0
0
0
0
Memaparkan 24 daripada 327